DMLS Ti-6Al-4V ELI Titanium3D printed metal (DMLS)
Plastic PEEKBulk polymer (molded or machined)
MechanicalDMLS Ti-6Al-4V ELI TitaniumPlastic PEEK
Yield strength1,100MPa111.2x stronger98MPa2
Ultimate tensile strength1,270MPa1not stated (yield given)
Compressive strengthnot sourced125MPa2
Flexural strengthnot sourced165MPa2
Elongation at break8.7%125%22.87x more ductile
Young's modulus (stiffness)same maker and process110GPa327.5x stiffer4GPa2
Density4,400kg/m³11,300kg/m³23.38x lighter
Strength to weight250kN·m/kg3.32x higher75.4kN·m/kg
Stiffness to weight25MN·m/kg8.13x higher3.08MN·m/kg
Poisson's ratiowrought TIMETAL 6-40.34240.385
Shear modulus41GPa28.3x stiffer in shear1.45GPa
Bulk modulus116GPa20.9x higher5.56GPa
Speed of sound5,000m/s2.85x faster1,754m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS Ti-6Al-4V ELI TitaniumPlastic PEEK
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS Ti-6Al-4V ELI TitaniumPlastic PEEK
Strength against densityHigher and further left: stronger for its weight
ThermalDMLS Ti-6Al-4V ELI TitaniumPlastic PEEK
Thermal conductivitybase material6.6W/m·K622.8x more heat through a fin0.29W/m·K2
Thermal expansionmean 25-100 °C9µm/m·K76.11x less55µm/m·K2
100 mm part over a 50 °C swing45µm growth6.11x less275µm growth
Specific heatbase material580J/kg·K62,200J/kg·K83.79x higher
Heats up and cools (diffusivity)2.59mm²/s25.5x faster0.101mm²/s
Thermal shock resistance4,825W/m60.2x more resistant80.1W/m
Melting pointmelting range1,630–1,650°C4343°C2
Glass transitionnot sourcedonset143°C2
Max service temperaturenot sourcedUL 746B RTI240°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS Ti-6Al-4V ELI TitaniumPlastic PEEK
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS Ti-6Al-4V ELI TitaniumPlastic PEEK
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources8 documents: EOS GmbH, Victrex, TIMET
DMLS Ti-6Al-4V ELI Titanium
EOS Titanium Ti64ELI (powder 9011-0040; ASTM F136/F3001, i.e. Grade 23) on EOS M400 SF, parameter set Ti64ELI_030_FlexM400_100, 30 µm, as built; ISO 6892-1 A14
Plastic PEEK
Victrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)
  1. 1
    EOS Titanium Ti64ELI Material Data Sheet, M 290 and M 400EOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Yield strength: typical, as built, average of horizontal + vertical (M400)DMLS Ti-6Al-4V ELI Titanium · Ultimate tensile strength: typical, as built, average of horizontal + vertical (M400)DMLS Ti-6Al-4V ELI Titanium · Elongation at break: typical at break, as built (M400)DMLS Ti-6Al-4V ELI Titanium · Density: typical part density (ISO 3369), M400
  2. 2
    VICTREX PEEK 450G Technical Data SheetVictrexPlastic PEEK · Yield strength: typical, tensile yieldPlastic PEEK · Compressive strength: typical, 23 CPlastic PEEK · Flexural strength: typical, flexural stress at yield, 23 CPlastic PEEK · Elongation at break: typical, at breakPlastic PEEK · Young's modulus (stiffness): typical (nominal)Plastic PEEK · Density: typical (crystalline)Plastic PEEK · Thermal conductivity: typical, average, 23 CPlastic PEEK · Thermal expansion: average of flow/cross-flow, below Tg (<143 C)Plastic PEEK · Melting point: typical, DSCPlastic PEEK · Glass transition: onset (midpoint 150 C)Plastic PEEK · Max service temperature: UL 746B RTI, mechanical strength (continuous use index)
  3. 3
    EOS Titanium Ti64 Material Data Sheet, M 290 (2022)EOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Young's modulus (stiffness): same maker and process, sibling grade: EOS Titanium Ti64 (Grade 5) on EOS M 290, as built, XY and Z, typical
  4. 4
    TIMETAL 6-4 PropertiesTIMETarchived copyDMLS Ti-6Al-4V ELI Titanium · Poisson's ratio: wrought TIMETAL 6-4 (TIMET measurement, mean of 10); composition-level, not DMLS-measuredDMLS Ti-6Al-4V ELI Titanium · Melting point: melting range, wrought TIMETAL 6-4 (composition-level)
  5. 5
    VICTREX PEEK for Use in Fluid Management (2020)VictrexPlastic PEEK · Poisson's ratio: typical
  6. 6
    TIMETAL 6-4 Data SheetTIMETarchived copyDMLS Ti-6Al-4V ELI Titanium · Thermal conductivity: base material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °CDMLS Ti-6Al-4V ELI Titanium · Specific heat: base material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
  7. 7
    EOS Titanium Ti64 Grade 23 Material Data SheetEOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Thermal expansion: mean 25-100 °C, ASTM E228; EOS Ti64 Grade 23 (=ELI) on EOS M 290 40 µm; condition not stated (sheet's mechanical data are heat treated)
  8. 8
    VICTREX PEEK 450G Technical Data Sheet (2012)Victrexarchived copyPlastic PEEK · Specific heat: typical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS Ti-6Al-4V ELI Titanium is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is DMLS Ti-6Al-4V ELI Titanium stronger than Plastic PEEK?

DMLS Ti-6Al-4V ELI Titanium is stronger: its yield strength is 1,100 MPa against 98 MPa for Plastic PEEK (11.2x).

Which is lighter, DMLS Ti-6Al-4V ELI Titanium or Plastic PEEK?

Plastic PEEK is lighter: 1,300 kg/m³ against 4,400 kg/m³ for DMLS Ti-6Al-4V ELI Titanium.

Which is stiffer, DMLS Ti-6Al-4V ELI Titanium or Plastic PEEK?

DMLS Ti-6Al-4V ELI Titanium is stiffer: Young's modulus 110 GPa against 4 GPa for Plastic PEEK, so the same part in DMLS Ti-6Al-4V ELI Titanium deflects less under the same load.

Which is lighter for the same job, DMLS Ti-6Al-4V ELI Titanium or Plastic PEEK?

For the same stiffness or strength: DMLS Ti-6Al-4V ELI Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam; Plastic PEEK is lighter for a stiff panel or plate, strong panel or plate.

Part that must beDMLS Ti-6Al-4V ELI TitaniumPlastic PEEK
Stiff rod or tie (tension)lighter8.13x heavier
Stiff beam (bending)lighter1.55x heavier
Stiff panel or plate12% heavierlighter
Strong rod or tielighter3.32x heavier
Strong beamlighter48% heavier
Strong panel or plate1% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, DMLS Ti-6Al-4V ELI Titanium or Plastic PEEK?

Plastic PEEK stretches further before it breaks: 25% elongation at break against 8.7% for DMLS Ti-6Al-4V ELI Titanium.

Thermal

Which conducts heat better, DMLS Ti-6Al-4V ELI Titanium or Plastic PEEK?

DMLS Ti-6Al-4V ELI Titanium conducts heat better: 6.6 W/m·K against 0.29 W/m·K for Plastic PEEK.

Which expands less with temperature?

DMLS Ti-6Al-4V ELI Titanium expands less: 9 µm/m·K against 55 µm/m·K for Plastic PEEK.