Materials / Compare

Drywall vs. Plastic Nylon

Compare Drywall vs. Plastic Nylon strength, stiffness, weight and thermal properties.

DrywallNatural
Plastic Nylon3D printed (FDM)
MechanicalDrywallPlastic Nylon
Yield strengthnot given (tensile used)63.1MPa1
Ultimate tensile strength1–2MPa263.1MPa1
Compressive strength2.4MPa3not sourced
Flexural strengthnot sourced82.9MPa1
Elongation at breaknot sourcednot sourced
Young's modulus (stiffness)1–2GPa22.33GPa1
Densitynot sourced1,140kg/m³1
Strength to weightnot sourced55.4kN·m/kg
Stiffness to weightnot sourced2.04MN·m/kg
Poisson's rationot sourcedbase material0.44
Shear modulusnot sourced0.833GPa
Bulk modulusnot sourced3.89GPa
Speed of soundnot sourced1,430m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPURubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon
Strength against densityHigher and further left: stronger for its weight
ThermalDrywallPlastic Nylon
Thermal conductivitynot sourcedbase material0.33W/m·K5
Thermal expansion16.7µm/m·K3base material98–102µm/m·K5
100 mm part over a 50 °C swing83.5µm growth5.99x less500µm growth
Specific heat1,090J/kg·K3base material1,700J/kg·K51.56x higher
Heats up and cools (diffusivity)not sourced0.17mm²/s
Thermal shock resistancenot sourced53.6W/m
Melting pointnot sourced188°C1
Glass transitionnot sourced55.1°C1
Max service temperature52°C6HDT 0.455 MPa89.2°C1
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources6 documents: UltiMaker, USDA Forest Products Laboratory, Gypsum Association, Covestro, BASF, USG
Drywall
1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittal
Plastic Nylon
Ultimaker Nylon, 3D-printed specimens, XY (flat), conditioned >=24 h at room temperature; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v2.00, April 20, 2022.
  1. 1
    Ultimaker Nylon Technical Data Sheet, v5.00UltiMakerarchived copyPlastic Nylon · Yield strength: typicalPlastic Nylon · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic Nylon · Flexural strength: typicalPlastic Nylon · Young's modulus (stiffness): typicalPlastic Nylon · Density: typicalPlastic Nylon · Melting point: typicalPlastic Nylon · Glass transition: typicalPlastic Nylon · Max service temperature: HDT 0.455 MPa (printed specimens)
  2. 2
    Mechanical Properties of Gypsum Board at Elevated TemperaturesUSDA Forest Products LaboratoryDrywall · Ultimate tensile strength: ambient range reported in review (Australian studies)Drywall · Young's modulus (stiffness): ambient range reported in review (Australian studies)
  3. 3
    GA-235-2023 Gypsum Board Typical Mechanical and Physical PropertiesGypsum AssociationDrywall · Compressive strength: typical, 70 F / 50% RHDrywall · Thermal expansion: typical, unrestrained, 3.3-32 CDrywall · Specific heat: typical (from ASHRAE Handbook of Fundamentals, per GA)
  4. 4
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
  5. 5
    Ultramid (PA) Product RangeBASFPlastic Nylon · Thermal conductivity: base material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)Plastic Nylon · Thermal expansion: base material: unreinforced BASF Ultramid PA66 (A3K, 98) and PA6 (B3S, 102), 23-55 CPlastic Nylon · Specific heat: base material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)
  6. 6
    Sheetrock Brand UltraLight Panels Submittal Sheet (WB2501)USGarchived copyDrywall · Max service temperature: manufacturer sustained-exposure limit

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Drywall stronger than Plastic Nylon?

Plastic Nylon is stronger: its yield strength is 63.1 MPa against tensile strength 1.5 MPa for Drywall (42.1x).

Which is stiffer, Drywall or Plastic Nylon?

Plastic Nylon is stiffer: Young's modulus 2.33 GPa against 1.5 GPa for Drywall, so the same part in Plastic Nylon deflects less under the same load.

Thermal

Which expands less with temperature?

Drywall expands less: 16.7 µm/m·K against 100 µm/m·K for Plastic Nylon.