Materials / Compare

FDM ASA vs. Plastic PPS GF40

Compare FDM ASA vs. Plastic PPS GF40 strength, stiffness, weight and thermal properties.

Change either side
FDM ASA3D printed (FDM)
Plastic PPS GF40Bulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength37MPasourcetypical195MPasourcetensile strength, 5 mm/min
Flexural strength65MPasourcetypical285MPasourceflexural strength at break
Elongation at break9.2%sourcetypical1.9%sourcestrain at break, 5 mm/min
Young's modulus (stiffness)2.45GPasourcetypical14.7GPasourcetypical, 1 mm/min
Density1,050kg/m³sourcetypical1.57x lighter1,650kg/m³sourcetypical
Strength to weight35.2kN·m/kg118kN·m/kg3.35x higher
Stiffness to weight2.33MN·m/kg8.91MN·m/kg3.82x higher
Poisson's rationot sourced0.35sourceglass-reinforced Fortron PPS (class value, not grade-specific)
Shear modulusnot sourced5.44GPa
Bulk modulusnot sourced16.3GPa
Speed of sound1,528m/s2,985m/s
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Luran S 777K injection-molding ASA, typical0.2W/m·Ksource40% glass-reinforced Fortron, 25 °C (not grade-specific)
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Luran S 777K injection-molding ASA, range12µm/m·Ksourceparallel (flow), mean -50 to 90 °C
100 mm part over a 50 °C swing475µm growth60µm growth7.92x less
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistancenot sourced144W/m
Melting pointnot sourced280°CsourceDSC, 10 °C/min
Glass transitionnot sourced90°CsourceDSC, 10 °C/min
Max service temperature92°CsourceHDT 1.8 MPa270°CsourceHDT 1.8 MPa2.93x hotter
Values forBambu Lab ASA, TDS V3.0, printed specimens X-Y; nozzle 260 °C, bed 80 °C, 200 mm/s, 100% infill; annealed and dried 80 °C for 12 h before testing.Celanese Fortron 1140L4 (PPS, 40% glass fibre), injection moulding; FORTRON PPS Short-Term Properties Guide (PPS-012, 2016); thermal conductivity and Poisson for 40% glass-reinforced Fortron from the Fortron PPS Design Manual (PPS-050, 2013).

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM ASA is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is FDM ASA stronger than Plastic PPS GF40?

Plastic PPS GF40 is stronger: its tensile strength is 195 MPa against 37 MPa for FDM ASA (5.27x).

Which is lighter, FDM ASA or Plastic PPS GF40?

FDM ASA is lighter: 1,050 kg/m³ against 1,650 kg/m³ for Plastic PPS GF40.

Which is stiffer, FDM ASA or Plastic PPS GF40?

Plastic PPS GF40 is stiffer: Young's modulus 14.7 GPa against 2.45 GPa for FDM ASA, so the same part in Plastic PPS GF40 deflects less under the same load.

Which is lighter for the same job, FDM ASA or Plastic PPS GF40?

For the same stiffness or strength: Plastic PPS GF40 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beFDM ASAPlastic PPS GF40
Stiff rod or tie (tension)3.82x heavierlighter
Stiff beam (bending)1.56x heavierlighter
Stiff panel or plate16% heavierlighter
Strong rod or tie3.35x heavierlighter
Strong beam1.93x heavierlighter
Strong panel or plate46% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which handles higher temperatures, FDM ASA or Plastic PPS GF40?

Plastic PPS GF40 does: 270 °C against 92 °C for FDM ASA, both HDT 1.8 MPa.

Which conducts heat better, FDM ASA or Plastic PPS GF40?

Plastic PPS GF40 conducts heat better: 0.2 W/m·K against 0.17 W/m·K for FDM ASA.

Which expands less with temperature?

Plastic PPS GF40 expands less: 12 µm/m·K against 95 µm/m·K for FDM ASA.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic LCP GF30FDM ASAPlastic PPS GF40
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic LCP GF30FDM ASAPlastic PPS GF40
Strength against density

Related comparisons