Materials / Compare

FDM PAHT-CF vs. FDM Polycarbonate

Compare FDM PAHT-CF vs. FDM Polycarbonate strength, stiffness, weight and thermal properties.

Change either side
FDM PAHT-CF3D printed (FDM)
FDM Polycarbonate3D printed (FDM)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)53.3MPasourcetypical
Ultimate tensile strength92MPasourcetypical53.3MPasourcetypical, peak stress (= stress at yield)
Flexural strength125MPasourcetypical40% stronger in bending89.4MPasourcetypical
Elongation at break8.4%sourcetypical9.2%sourcetypical
Young's modulus (stiffness)3.86GPasourcetypical1.61x stiffer2.39GPasourcetypical
Density1,060kg/m³sourcetypical1,180–1,200kg/m³sourcerange
Strength to weight86.8kN·m/kg1.94x higher44.8kN·m/kg
Stiffness to weight3.64MN·m/kg1.81x higher2.01MN·m/kg
Poisson's rationot sourced0.38sourcebase material: polycarbonate family typical (Covestro Part and Mold Design guide, Table 3-1)
Shear modulusnot sourced0.867GPa
Bulk modulusnot sourced3.33GPa
Speed of sound1,908m/s1,418m/s
Thermal
Thermal conductivitynot sourced0.2W/m·Ksourcebase material: Covestro Makrolon 2405 injection-molding PC, typical, through-plane, 23 °C
Thermal expansionnot sourced65µm/m·Ksourcebase material: Covestro Makrolon 2405 injection-molding PC, typical, 23-55 °C, parallel
100 mm part over a 50 °C swingnot sourced325µm growth
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistancenot sourced42.5W/m
Melting point225°Csourcetypicalnot sourced
Glass transition70°Csourcetypical108°Csourcetypical
Max service temperature170°CsourceHDT 1.8 MPa105°CsourceHDT 0.455 MPa (printed specimens)
Values forBambu Lab PAHT-CF, TDS V3.0, printed specimens X-Y, dry state; nozzle 290 °C, bed 100 °C, 100 mm/s, 100% infill; annealed and dried 80 °C for 12 h before testing.Ultimaker PC, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 20, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM PAHT-CF and FDM Polycarbonate are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is FDM PAHT-CF stronger than FDM Polycarbonate?

FDM PAHT-CF is stronger: its tensile strength is 92 MPa against yield strength 53.3 MPa for FDM Polycarbonate (1.73x).

Which is lighter, FDM PAHT-CF or FDM Polycarbonate?

FDM PAHT-CF is lighter: 1,060 kg/m³ against 1,190 kg/m³ for FDM Polycarbonate.

Which is stiffer, FDM PAHT-CF or FDM Polycarbonate?

FDM PAHT-CF is stiffer: Young's modulus 3.86 GPa against 2.39 GPa for FDM Polycarbonate, so the same part in FDM PAHT-CF deflects less under the same load.

Which is lighter for the same job, FDM PAHT-CF or FDM Polycarbonate?

For the same stiffness or strength: FDM PAHT-CF is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beFDM PAHT-CFFDM Polycarbonate
Stiff rod or tie (tension)lighter1.81x heavier
Stiff beam (bending)lighter43% heavier
Stiff panel or platelighter32% heavier
Strong rod or tielighter1.94x heavier
Strong beamlighter1.62x heavier
Strong panel or platelighter47% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelFDM PAHT-CFFDM Polycarbonate
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickFDM PAHT-CFFDM Polycarbonate
Strength against density

Related comparisons