Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ31B-H24 · Young's modulus (stiffness): typical (handbook physical constant)Magnesium AZ31B-H24 · Density: nominalMagnesium AZ31B-H24 · Poisson's ratio: typical (handbook physical constant)Magnesium AZ31B-H24 · Max service temperature: stated application limit
4
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon PA6 · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Magnesium AZ31B-H24 stronger than Plastic Nylon PA6?
Magnesium AZ31B-H24 is stronger: its yield strength is 220 MPa against 90 MPa for Plastic Nylon PA6 (2.44x).
Which is lighter, Magnesium AZ31B-H24 or Plastic Nylon PA6?
Plastic Nylon PA6 is lighter: 1,130 kg/m³ against 1,769 kg/m³ for Magnesium AZ31B-H24.
Which is stiffer, Magnesium AZ31B-H24 or Plastic Nylon PA6?
Magnesium AZ31B-H24 is stiffer: Young's modulus 44.8 GPa against 3.5 GPa for Plastic Nylon PA6, so the same part in Magnesium AZ31B-H24 deflects less under the same load.
Which is lighter for the same job, Magnesium AZ31B-H24 or Plastic Nylon PA6?
For the same stiffness or strength: Magnesium AZ31B-H24 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam.
Part that must be
Magnesium AZ31B-H24
Plastic Nylon PA6
Stiff rod or tie (tension)
lighter
8.18x heavier
Stiff beam (bending)
lighter
2.29x heavier
Stiff panel or plate
lighter
49% heavier
Strong rod or tie
lighter
1.56x heavier
Strong beam
lighter
16% heavier
Strong panel or plate
about equal
about equal
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Magnesium AZ31B-H24 or Plastic Nylon PA6?
Magnesium AZ31B-H24 stretches further before it breaks: 13% elongation at break against 10% for Plastic Nylon PA6.
Thermal
Which handles higher temperatures, Magnesium AZ31B-H24 or Plastic Nylon PA6?
Magnesium AZ31B-H24 does: 149 °C against 87 °C for Plastic Nylon PA6.
Which conducts heat better, Magnesium AZ31B-H24 or Plastic Nylon PA6?
Magnesium AZ31B-H24 conducts heat better: 76.9 W/m·K against 0.33 W/m·K for Plastic Nylon PA6.
Which expands less with temperature?
Magnesium AZ31B-H24 expands less: 26.8 µm/m·K against 102 µm/m·K for Plastic Nylon PA6.