Materials / Compare

Magnesium AZ31B-H24 vs. Plastic PMMA

Compare Magnesium AZ31B-H24 vs. Plastic PMMA strength, stiffness, weight and thermal properties.

Magnesium AZ31B-H24Wrought
Plastic PMMABulk polymer (molded or machined)
MechanicalMagnesium AZ31B-H24Plastic PMMA
Yield strength220MPa1not given (tensile used)
Ultimate tensile strength290MPa13.63x stronger80MPa2
Compressive strengthnot sourced110MPa2
Flexural strengthnot sourced115MPa2
Elongation at break13%12.36x more ductile5.5%2
Young's modulus (stiffness)44.8GPa313.6x stiffer3.3GPa2
Density1,769kg/m³31,190kg/m³249% lighter
Strength to weight124kN·m/kg1.85x higher67.2kN·m/kg
Stiffness to weight25.3MN·m/kg9.13x higher2.77MN·m/kg
Poisson's ratio0.3530.372
Shear modulus16.6GPa13.8x stiffer in shear1.2GPa
Bulk modulus49.8GPa11.8x higher4.23GPa
Speed of sound5,032m/s3.02x faster1,665m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ31B-H24Plastic PMMA
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ31B-H24Plastic PMMA
Strength against densityHigher and further left: stronger for its weight
ThermalMagnesium AZ31B-H24Plastic PMMA
Thermal conductivity76.9W/m·K1405x more heat through a fin0.19W/m·K2
Thermal expansion26.8µm/m·K12.61x less0-50 °C70µm/m·K2
100 mm part over a 50 °C swing134µm growth2.61x less350µm growth
Specific heat1,040J/kg·K11,470J/kg·K241% higher
Heats up and cools (diffusivity)41.8mm²/s385x faster0.109mm²/s
Thermal shock resistance9,159W/m221x more resistant41.5W/m
Max service temperature149°C380°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ31B-H24Plastic PMMA
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ31B-H24Plastic PMMA
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Magnesium Elektron, Röhm, U.S. Department of Defense
Magnesium AZ31B-H24
AZ31B-H24 sheet 0.016-0.062 in., MIL-HDBK-5J Table 4.2.1.0(b) (AMS 4377); strengths are S-basis MINIMUMS
Plastic PMMA
Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)
  1. 1
    Elektron AZ31B Sheet, Plate & Coil (Datasheet 482)Magnesium Elektronarchived copyMagnesium AZ31B-H24 · Yield strength: typical, H24, 0.5-6 mm, 0.2 % proof stressMagnesium AZ31B-H24 · Ultimate tensile strength: typical, H24, 0.5-6 mmMagnesium AZ31B-H24 · Elongation at break: typical, H24, 0.5-6 mm, gauge 5.65√AMagnesium AZ31B-H24 · Thermal conductivity: typical (temper/temperature not stated)Magnesium AZ31B-H24 · Thermal expansion: typical (temperature range not stated)Magnesium AZ31B-H24 · Specific heat: typical
  2. 2
    PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1)Röhmarchived copyPlastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ31B-H24 · Young's modulus (stiffness): typical (handbook physical constant)Magnesium AZ31B-H24 · Density: nominalMagnesium AZ31B-H24 · Poisson's ratio: typical (handbook physical constant)Magnesium AZ31B-H24 · Max service temperature: stated application limit

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Magnesium AZ31B-H24 stronger than Plastic PMMA?

Magnesium AZ31B-H24 is stronger: its yield strength is 220 MPa against tensile strength 80 MPa for Plastic PMMA (2.75x).

Which is lighter, Magnesium AZ31B-H24 or Plastic PMMA?

Plastic PMMA is lighter: 1,190 kg/m³ against 1,769 kg/m³ for Magnesium AZ31B-H24.

Which is stiffer, Magnesium AZ31B-H24 or Plastic PMMA?

Magnesium AZ31B-H24 is stiffer: Young's modulus 44.8 GPa against 3.3 GPa for Plastic PMMA, so the same part in Magnesium AZ31B-H24 deflects less under the same load.

Which is lighter for the same job, Magnesium AZ31B-H24 or Plastic PMMA?

For the same stiffness or strength: Magnesium AZ31B-H24 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beMagnesium AZ31B-H24Plastic PMMA
Stiff rod or tie (tension)lighter9.13x heavier
Stiff beam (bending)lighter2.48x heavier
Stiff panel or platelighter1.6x heavier
Strong rod or tielighter1.85x heavier
Strong beamlighter32% heavier
Strong panel or platelighter12% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Magnesium AZ31B-H24 or Plastic PMMA?

Magnesium AZ31B-H24 stretches further before it breaks: 13% elongation at break against 5.5% for Plastic PMMA.

Thermal

Which conducts heat better, Magnesium AZ31B-H24 or Plastic PMMA?

Magnesium AZ31B-H24 conducts heat better: 76.9 W/m·K against 0.19 W/m·K for Plastic PMMA.

Which expands less with temperature?

Magnesium AZ31B-H24 expands less: 26.8 µm/m·K against 70 µm/m·K for Plastic PMMA.