Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Celanese GUR 4120 (avg. molecular weight 4.7x10^6 g/mol), typical values on compression-molded specimens; CTE and thermal conductivity from Celanese's generic UHMWPE guide (grade not named)
1
Elektron AZ31B Sheet, Plate & Coil (Datasheet 482)Magnesium Elektronarchived copyMagnesium AZ31B-H24 · Yield strength: typical, H24, 0.5-6 mm, 0.2 % proof stressMagnesium AZ31B-H24 · Ultimate tensile strength: typical, H24, 0.5-6 mmMagnesium AZ31B-H24 · Elongation at break: typical, H24, 0.5-6 mm, gauge 5.65√AMagnesium AZ31B-H24 · Thermal conductivity: typical (temper/temperature not stated)Magnesium AZ31B-H24 · Thermal expansion: typical (temperature range not stated)Magnesium AZ31B-H24 · Specific heat: typical
2
GUR UHMW-PE Overview (GUR-015)CelanesePlastic UHMWPE · Yield strength: typical, tensile stress at yield ISO 527, 50 mm/minPlastic UHMWPE · Ultimate tensile strength: typical, tensile stress at break ISO 527, 50 mm/minPlastic UHMWPE · Elongation at break: typical, nominal elongation at break ISO 527Plastic UHMWPE · Young's modulus (stiffness): typical, tensile modulus ISO 527, 1 mm/minPlastic UHMWPE · Density: typicalPlastic UHMWPE · Melting point: DSC 10 K/minPlastic UHMWPE · Max service temperature: recommended max constant operating temperature
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ31B-H24 · Young's modulus (stiffness): typical (handbook physical constant)Magnesium AZ31B-H24 · Density: nominalMagnesium AZ31B-H24 · Poisson's ratio: typical (handbook physical constant)Magnesium AZ31B-H24 · Max service temperature: stated application limit
4
GUR UHMW-PE Polymer Guide (GUR-003)Celanesearchived copyPlastic UHMWPE · Thermal conductivity: typical, unfilled (narrative value, generic Celanese UHMWPE)Plastic UHMWPE · Thermal expansion: typical, 20 to 100 °C (generic Celanese UHMWPE)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Magnesium AZ31B-H24 stronger than Plastic UHMWPE?
Magnesium AZ31B-H24 is stronger: its yield strength is 220 MPa against 20 MPa for Plastic UHMWPE (11x).
Which is lighter, Magnesium AZ31B-H24 or Plastic UHMWPE?
Plastic UHMWPE is lighter: 930 kg/m³ against 1,769 kg/m³ for Magnesium AZ31B-H24.
Which is stiffer, Magnesium AZ31B-H24 or Plastic UHMWPE?
Magnesium AZ31B-H24 is stiffer: Young's modulus 44.8 GPa against 0.66 GPa for Plastic UHMWPE, so the same part in Magnesium AZ31B-H24 deflects less under the same load.
Which is lighter for the same job, Magnesium AZ31B-H24 or Plastic UHMWPE?
For the same stiffness or strength: Magnesium AZ31B-H24 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Magnesium AZ31B-H24
Plastic UHMWPE
Stiff rod or tie (tension)
lighter
35.7x heavier
Stiff beam (bending)
lighter
4.33x heavier
Stiff panel or plate
lighter
2.14x heavier
Strong rod or tie
lighter
5.78x heavier
Strong beam
lighter
2.6x heavier
Strong panel or plate
lighter
1.74x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Magnesium AZ31B-H24 or Plastic UHMWPE?
Plastic UHMWPE stretches further before it breaks: 465% elongation at break against 13% for Magnesium AZ31B-H24.
Thermal
Which handles higher temperatures, Magnesium AZ31B-H24 or Plastic UHMWPE?
Magnesium AZ31B-H24 does: 149 °C against 80 °C for Plastic UHMWPE.
Which conducts heat better, Magnesium AZ31B-H24 or Plastic UHMWPE?
Magnesium AZ31B-H24 conducts heat better: 76.9 W/m·K against 0.4 W/m·K for Plastic UHMWPE.
Which expands less with temperature?
Magnesium AZ31B-H24 expands less: 26.8 µm/m·K against 200 µm/m·K for Plastic UHMWPE.