Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.
1
Elektron AZ31B Sheet, Plate & Coil (Datasheet 482)Magnesium Elektronarchived copyMagnesium AZ31B-H24 · Yield strength: typical, H24, 0.5-6 mm, 0.2 % proof stressMagnesium AZ31B-H24 · Ultimate tensile strength: typical, H24, 0.5-6 mmMagnesium AZ31B-H24 · Elongation at break: typical, H24, 0.5-6 mm, gauge 5.65√AMagnesium AZ31B-H24 · Thermal conductivity: typical (temper/temperature not stated)Magnesium AZ31B-H24 · Thermal expansion: typical (temperature range not stated)Magnesium AZ31B-H24 · Specific heat: typical
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ31B-H24 · Young's modulus (stiffness): typical (handbook physical constant)Magnesium AZ31B-H24 · Density: nominalMagnesium AZ31B-H24 · Poisson's ratio: typical (handbook physical constant)Magnesium AZ31B-H24 · Max service temperature: stated application limit
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Magnesium AZ31B-H24 stronger than SLA Resin Elastic 50A?
Magnesium AZ31B-H24 is stronger: its yield strength is 220 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (64.7x).
Which is lighter, Magnesium AZ31B-H24 or SLA Resin Elastic 50A?
SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 1,769 kg/m³ for Magnesium AZ31B-H24.
Which is lighter for the same job, Magnesium AZ31B-H24 or SLA Resin Elastic 50A?
For the same stiffness or strength: Magnesium AZ31B-H24 is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Magnesium AZ31B-H24
SLA Resin Elastic 50A
Strong rod or tie
lighter
36.9x heavier
Strong beam
lighter
9.2x heavier
Strong panel or plate
lighter
4.59x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Magnesium AZ31B-H24 or SLA Resin Elastic 50A?
SLA Resin Elastic 50A stretches further before it breaks: 160% elongation at break against 13% for Magnesium AZ31B-H24.