Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
1
Elektron AZ31B Sheet, Plate & Coil (Datasheet 482)Magnesium Elektronarchived copyMagnesium AZ31B-H24 · Yield strength: typical, H24, 0.5-6 mm, 0.2 % proof stressMagnesium AZ31B-H24 · Ultimate tensile strength: typical, H24, 0.5-6 mmMagnesium AZ31B-H24 · Elongation at break: typical, H24, 0.5-6 mm, gauge 5.65√AMagnesium AZ31B-H24 · Thermal conductivity: typical (temper/temperature not stated)Magnesium AZ31B-H24 · Thermal expansion: typical (temperature range not stated)Magnesium AZ31B-H24 · Specific heat: typical
2
ATI 316, 316L, 317 and 317L Technical Data Sheet (2012)ATIarchived copyStainless Steel 316 · Yield strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Ultimate tensile strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Elongation at break: typical (representative), annealed, in 2 in. (51 mm)Stainless Steel 316 · Young's modulus (stiffness): typical, in tensionStainless Steel 316 · Density: typicalStainless Steel 316 · Thermal conductivity: 20–100 °CStainless Steel 316 · Thermal expansion: mean, 20–100 °CStainless Steel 316 · Specific heat: at 20 °CStainless Steel 316 · Melting point: melting rangeStainless Steel 316 · Max service temperature: oxidation (scaling) limit in air
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ31B-H24 · Young's modulus (stiffness): typical (handbook physical constant)Magnesium AZ31B-H24 · Density: nominalMagnesium AZ31B-H24 · Poisson's ratio: typical (handbook physical constant)Magnesium AZ31B-H24 · Max service temperature: stated application limit
4
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 316 · Poisson's ratio: design value (structural stainless steels)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Magnesium AZ31B-H24 stronger than Stainless Steel 316?
Stainless Steel 316 is stronger: its yield strength is 265 MPa against 220 MPa for Magnesium AZ31B-H24 (20%).
Which is lighter, Magnesium AZ31B-H24 or Stainless Steel 316?
Magnesium AZ31B-H24 is lighter: 1,769 kg/m³ against 8,027 kg/m³ for Stainless Steel 316.
Which is stiffer, Magnesium AZ31B-H24 or Stainless Steel 316?
Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 44.8 GPa for Magnesium AZ31B-H24, so the same part in Stainless Steel 316 deflects less under the same load.
Which is lighter for the same job, Magnesium AZ31B-H24 or Stainless Steel 316?
For the same stiffness or strength: Magnesium AZ31B-H24 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Magnesium AZ31B-H24
Stainless Steel 316
Stiff rod or tie (tension)
lighter
2% heavier
Stiff beam (bending)
lighter
2.15x heavier
Stiff panel or plate
lighter
2.76x heavier
Strong rod or tie
lighter
3.77x heavier
Strong beam
lighter
4.01x heavier
Strong panel or plate
lighter
4.13x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Magnesium AZ31B-H24 or Stainless Steel 316?
Stainless Steel 316 stretches further before it breaks: 61% elongation at break against 13% for Magnesium AZ31B-H24.
Thermal
Which conducts heat better, Magnesium AZ31B-H24 or Stainless Steel 316?
Magnesium AZ31B-H24 conducts heat better: 76.9 W/m·K against 14.6 W/m·K for Stainless Steel 316.
Which expands less with temperature?
Stainless Steel 316 expands less: 16.5 µm/m·K against 26.8 µm/m·K for Magnesium AZ31B-H24.