Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: Magnesium Elektron, Formlabs, U.S. Department of Defense
Magnesium AZ91D
ELEKTRON AZ91D magnesium die-casting alloy, as cast; Magnesium Elektron datasheet 475 (7/01), typical properties; Poisson from MIL-HDBK-5J for AZ91C castings.
SLA Resin Elastic 50A
Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.
1
Elektron Die Casting Alloys (Datasheet 475)Magnesium Elektronarchived copyMagnesium AZ91D · Yield strength: typical, 0.2% tensile yield, ambient temperatureMagnesium AZ91D · Ultimate tensile strength: typical, ambient temperatureMagnesium AZ91D · Elongation at break: typical, ambient temperatureMagnesium AZ91D · Young's modulus (stiffness): typicalMagnesium AZ91D · Density: typicalMagnesium AZ91D · Thermal conductivity: typicalMagnesium AZ91D · Thermal expansion: typical, temperature range not statedMagnesium AZ91D · Specific heat: typicalMagnesium AZ91D · Melting point: melting range
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ91D · Poisson's ratio: base material: AZ91C casting (MIL-HDBK-5J handbook physical constant)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Magnesium AZ91D stronger than SLA Resin Elastic 50A?
Magnesium AZ91D is stronger: its yield strength is 150 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (44.1x).
Which is lighter, Magnesium AZ91D or SLA Resin Elastic 50A?
SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 1,810 kg/m³ for Magnesium AZ91D.
Which is lighter for the same job, Magnesium AZ91D or SLA Resin Elastic 50A?
For the same stiffness or strength: Magnesium AZ91D is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Magnesium AZ91D
SLA Resin Elastic 50A
Strong rod or tie
lighter
24.6x heavier
Strong beam
lighter
6.97x heavier
Strong panel or plate
lighter
3.71x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Magnesium AZ91D or SLA Resin Elastic 50A?
SLA Resin Elastic 50A stretches further before it breaks: 160% elongation at break against 3% for Magnesium AZ91D.