Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Magnesium Elektron, Formlabs, U.S. Department of Defense
Magnesium AZ91D
ELEKTRON AZ91D magnesium die-casting alloy, as cast; Magnesium Elektron datasheet 475 (7/01), typical properties; Poisson from MIL-HDBK-5J for AZ91C castings.
SLA Resin Standard
Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.
1
Elektron Die Casting Alloys (Datasheet 475)Magnesium Elektronarchived copyMagnesium AZ91D · Yield strength: typical, 0.2% tensile yield, ambient temperatureMagnesium AZ91D · Ultimate tensile strength: typical, ambient temperatureMagnesium AZ91D · Elongation at break: typical, ambient temperatureMagnesium AZ91D · Young's modulus (stiffness): typicalMagnesium AZ91D · Density: typicalMagnesium AZ91D · Thermal conductivity: typicalMagnesium AZ91D · Thermal expansion: typical, temperature range not statedMagnesium AZ91D · Specific heat: typicalMagnesium AZ91D · Melting point: melting range
2
Clear Resin V5 Technical Data Sheet (2024)Formlabsarchived copySLA Resin Standard · Ultimate tensile strength: typicalSLA Resin Standard · Flexural strength: typicalSLA Resin Standard · Elongation at break: typicalSLA Resin Standard · Young's modulus (stiffness): typicalSLA Resin Standard · Max service temperature: HDT 1.8 MPa
3
Clear Resin V5 Technical Data Sheet (web edition)FormlabsSLA Resin Standard · Density: typical, post-cured (same for 5 min ambient and 15 min at 60 °C), ASTM D792
4
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ91D · Poisson's ratio: base material: AZ91C casting (MIL-HDBK-5J handbook physical constant)
5
Thermal Properties of Selected Formlabs SLA ResinsFormlabsSLA Resin Standard · Thermal conductivity: typical, post-cured, ASTM E1530SLA Resin Standard · Thermal expansion: mean -30 to 140 °C, post-cured (5 min ambient cure), TMA ASTM E831SLA Resin Standard · Specific heat: typical, 25 °C, post-cured (5 min ambient cure), DSC ASTM E1269
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Magnesium AZ91D stronger than SLA Resin Standard?
Magnesium AZ91D is stronger: its yield strength is 150 MPa against tensile strength 60 MPa for SLA Resin Standard (2.5x).
Which is lighter, Magnesium AZ91D or SLA Resin Standard?
SLA Resin Standard is lighter: 1,210 kg/m³ against 1,810 kg/m³ for Magnesium AZ91D.
Which is stiffer, Magnesium AZ91D or SLA Resin Standard?
Magnesium AZ91D is stiffer: Young's modulus 45 GPa against 2.75 GPa for SLA Resin Standard, so the same part in Magnesium AZ91D deflects less under the same load.
Which is lighter for the same job, Magnesium AZ91D or SLA Resin Standard?
For the same stiffness or strength: Magnesium AZ91D is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Magnesium AZ91D
SLA Resin Standard
Stiff rod or tie (tension)
lighter
10.9x heavier
Stiff beam (bending)
lighter
2.7x heavier
Stiff panel or plate
lighter
1.7x heavier
Strong rod or tie
lighter
1.67x heavier
Strong beam
lighter
23% heavier
Strong panel or plate
lighter
6% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Magnesium AZ91D or SLA Resin Standard?
SLA Resin Standard stretches further before it breaks: 8% elongation at break against 3% for Magnesium AZ91D.
Thermal
Which conducts heat better, Magnesium AZ91D or SLA Resin Standard?
Magnesium AZ91D conducts heat better: 72 W/m·K against 0.54 W/m·K for SLA Resin Standard.
Which expands less with temperature?
Magnesium AZ91D expands less: 25 µm/m·K against 114 µm/m·K for SLA Resin Standard.