Materials / Compare
Nickel Inconel 718 vs. Steel AISI 1018
Compare Nickel Inconel 718 vs. Steel AISI 1018 strength, stiffness, weight and thermal properties.
| Mechanical | Nickel Inconel 718 | Steel AISI 1018 |
|---|---|---|
| Yield strength | 1,207MPa13.24x stronger | producer-stated372MPa2 |
| Ultimate tensile strength | 1,389MPa13.15x stronger | producer-stated441MPa2 |
| Elongation at break | 20%133% more ductile | in 2 in15%2 |
| Young's modulus (stiffness) | 200GPa1 | base material200GPa3 |
| Density | 8,221kg/m³1 | base material7,861kg/m³3 |
| Strength to weight | 147kN·m/kg3.1x higher | 47.3kN·m/kg |
| Stiffness to weight | 24.3MN·m/kg | 25.4MN·m/kg5% higher |
| Poisson's ratio | 0.2941 | base material0.323 |
| Shear modulus | 77.3GPa2% stiffer in shear | 75.7GPa |
| Bulk modulus | 162GPa | 185GPa14% higher |
| Speed of sound | 4,932m/s | 5,043m/s2% faster |
| Thermal | Nickel Inconel 718 | Steel AISI 1018 |
|---|---|---|
| Thermal conductivity | 11.4W/m·K1 | base material51.9W/m·K3 |
| Thermal expansion | 13.2µm/m·K1 | base material12µm/m·K4 |
| 100 mm part over a 50 °C swing | 66µm growth | 60µm growth10% less |
| Specific heat | 435J/kg·K1 | base material486J/kg·K3 |
| Heats up and cools (diffusivity) | 3.19mm²/s | 13.6mm²/s4.26x faster |
| Thermal shock resistance | 3,680W/m | 5,473W/m49% more resistant |
| Melting point | melting range1,260–1,336°C1 | not sourced |
| Max service temperature | 704°C1 | not sourced |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources4 documents: Special Metals, Niagara LaSalle, U.S. Department of Defense, Ovako
- Nickel Inconel 718
- INCONEL alloy 718, standard grade, 1750 °F/1 hr anneal + 1325 °F/8 hr F.C. to 1150 °F aged; Special Metals bulletin SMC-045 typical values
- Steel AISI 1018
- AISI 1018 cold drawn bar (Niagara LaSalle, cold-finished bar producer)
- 1INCONEL alloy 718 (SMC-045)Special Metalsarchived copyNickel Inconel 718 · Yield strength: typical, 1.0 in. hot-rolled bar, 0.2% offsetNickel Inconel 718 · Ultimate tensile strength: typical, 1.0 in. barNickel Inconel 718 · Elongation at break: typical, 1.0 in. barNickel Inconel 718 · Young's modulus (stiffness): typical, 21 °C, annealed + agedNickel Inconel 718 · Density: nominal, annealed and agedNickel Inconel 718 · Poisson's ratio: typical, 21 °C, annealed + agedNickel Inconel 718 · Thermal conductivity: typical, 21 °C, annealed + aged (calculated from resistivity per footnote a)Nickel Inconel 718 · Thermal expansion: typical, mean 21-93 °C, annealed + agedNickel Inconel 718 · Specific heat: typical, 21 °CNickel Inconel 718 · Melting point: melting rangeNickel Inconel 718 · Max service temperature: upper use temperature stated by producer
- 21018 PropertiesNiagara LaSallearchived copySteel AISI 1018 · Yield strength: producer-stated, cold drawnSteel AISI 1018 · Ultimate tensile strength: producer-stated, cold drawnSteel AISI 1018 · Elongation at break: in 2 in (50.8 mm)
- 3MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 1018 · Young's modulus (stiffness): base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Density: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Poisson's ratio: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Thermal conductivity: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Specific heat: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
- 4S275JR Steel GradeOvakoSteel AISI 1018 · Thermal expansion: base material: unalloyed carbon steel, Ovako family table (S275JR, 'none alloyed structural steels', C <= 0.21%); mean 20-300 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Nickel Inconel 718 stronger than Steel AISI 1018?
Nickel Inconel 718 is stronger: its yield strength is 1,207 MPa against 372 MPa for Steel AISI 1018 (3.24x).
Which is lighter, Nickel Inconel 718 or Steel AISI 1018?
Steel AISI 1018 is lighter: 7,861 kg/m³ against 8,221 kg/m³ for Nickel Inconel 718.
Which is stiffer, Nickel Inconel 718 or Steel AISI 1018?
Nickel Inconel 718 is stiffer: Young's modulus 200 GPa against 200 GPa for Steel AISI 1018, so the same part in Nickel Inconel 718 deflects less under the same load.
Which is lighter for the same job, Nickel Inconel 718 or Steel AISI 1018?
For the same stiffness or strength: Nickel Inconel 718 is lighter for a strong rod or tie, strong beam, strong panel or plate; Steel AISI 1018 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.
| Part that must be | Nickel Inconel 718 | Steel AISI 1018 |
|---|---|---|
| Stiff rod or tie (tension) | 5% heavier | lighter |
| Stiff beam (bending) | 5% heavier | lighter |
| Stiff panel or plate | 5% heavier | lighter |
| Strong rod or tie | lighter | 3.1x heavier |
| Strong beam | lighter | 2.1x heavier |
| Strong panel or plate | lighter | 1.72x heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Nickel Inconel 718 or Steel AISI 1018?
Nickel Inconel 718 stretches further before it breaks: 20% elongation at break against 15% for Steel AISI 1018.
Thermal
Which conducts heat better, Nickel Inconel 718 or Steel AISI 1018?
Steel AISI 1018 conducts heat better: 51.9 W/m·K against 11.4 W/m·K for Nickel Inconel 718.
Which expands less with temperature?
Steel AISI 1018 expands less: 12 µm/m·K against 13.2 µm/m·K for Nickel Inconel 718.
Related comparisons
- Nickel Inconel 718 vs. Stainless Steel 17-4PH
- Nickel Inconel 718 vs. Steel AISI 4340
- Nickel Inconel 718 vs. DMLS 17-4PH Stainless Steel
- Nickel Inconel 718 vs. Steel AISI 1045
- Steel AISI 1018 vs. Steel
- Steel AISI 1018 vs. Steel A992
- Steel AISI 1018 vs. Stainless Steel 303
- Steel AISI 1018 vs. Stainless Steel 316