Materials / Compare

PCB Board FR-4, 2 copper planes vs. Plastic PMMA

Compare PCB Board FR-4, 2 copper planes vs. Plastic PMMA strength, stiffness, weight and thermal properties.

Change either side
PCB Board FR-4, 2 copper planesComposite
Plastic PMMABulk polymer (molded or machined)
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength246–385MPasourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction (ASTM D3039)80MPasourcetypical, 23 °C
Compressive strengthnot sourced110MPasourcecompressive yield stress, typical
Flexural strengthnot sourced115MPasourcetypical
Elongation at breaknot sourced5.5%sourcetypical
Young's modulus (stiffness)21.9–25.8GPasourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction (ASTM D790-15e2); the copper planes are left out3.3GPasourcetypical, short-term
Densitynot sourced1,190kg/m³sourcetypical
Strength to weightnot sourced67.2kN·m/kg
Stiffness to weightnot sourced2.77MN·m/kg
Poisson's ratio0.171–0.177sourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction0.37sourcetypical
Shear modulus10.2GPa8.44x stiffer in shear1.2GPa
Bulk modulus12.2GPa4.23GPa
Speed of soundnot sourced1,665m/s
Thermal
Thermal conductivitynot sourced0.19W/m·Ksourcetypical
Thermal expansion13–14µm/m·Ksourcethe bare laminate's (fr4-370hr), in-plane X/Y-axis, below Tg (IPC-TM-650 2.4.24C)70µm/m·Ksource0-50 °C
100 mm part over a 50 °C swing67.5µm growth5.19x less350µm growth
Specific heatnot sourced1,470J/kg·Ksourcetypical
Heats up and cools (diffusivity)not sourced0.109mm²/s
Thermal shock resistancenot sourced41.5W/m
Max service temperaturenot sourced80°Csourcemax. permanent service temperature
Values forA whole circuit board read as one orthotropic plate: the JEDEC high-K thermal test board (JESD51-7, "2s2p"), 0.062 in (1.575 mm) thick with two internal solid copper planes 0.0014 in (1 oz) thick, as Texas Instruments SZZA017A Table 1 gives it. Copper C110 and the Isola 370HR laminate from this library; the layers conduct in parallel along the board and in series through it (boardStackup.ts). Its two 0.0028 in trace layers cover little of the board and are left out; vias are ignored. Mechanical values are the bare laminate's.Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is PCB Board FR-4, 2 copper planes stronger than Plastic PMMA?

PCB Board FR-4, 2 copper planes is stronger: its tensile strength is 315 MPa against 80 MPa for Plastic PMMA (3.94x).

Which is stiffer, PCB Board FR-4, 2 copper planes or Plastic PMMA?

PCB Board FR-4, 2 copper planes is stiffer: Young's modulus 23.9 GPa against 3.3 GPa for Plastic PMMA, so the same part in PCB Board FR-4, 2 copper planes deflects less under the same load.

Which expands less with temperature?

PCB Board FR-4, 2 copper planes expands less: 13.5 µm/m·K against 70 µm/m·K for Plastic PMMA.

Among 73 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PMMA
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PMMA
Strength against density

Related comparisons