Materials / Compare

Plastic ABS vs. Rubber

Compare Plastic ABS vs. Rubber strength, stiffness, weight and thermal properties.

Change either side
Plastic ABS3D printed (FDM)
RubberBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength38.1MPasourcetypicalnot given (tensile used)
Ultimate tensile strength38.1MPasourcetypical, peak stress (= stress at yield)23MPasourcetypical
Flexural strength61.1MPasourcetypicalnot sourced
Elongation at break4.6%sourcetypical830%sourcetypical180x more ductile
Young's modulus (stiffness)1.96GPasourcetypicalnot sourced
Density1,100kg/m³sourcetypical960kg/m³sourcetypical (specific gravity)
Strength to weight34.6kN·m/kg45% higher24kN·m/kg
Stiffness to weight1.78MN·m/kgnot sourced
Poisson's ratio0.39sourcebase material: ABS family typical (Covestro Part and Mold Design guide, Table 3-1)0.5sourcegovernment (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible).
Shear modulus0.706GPanot sourced
Bulk modulus2.97GPanot sourced
Speed of sound1,336m/snot sourced
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, typical0.151W/m·Ksourcegovernment selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, rangenot sourced
100 mm part over a 50 °C swing475µm growthnot sourced
Specific heatnot sourced1,881J/kg·Ksourcegovernment (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C
Heats up and cools (diffusivity)not sourced0.0836mm²/s
Thermal shock resistance21.2W/mnot sourced
Glass transition101°Csourcetypicalnot sourced
Max service temperature86.6°CsourceHDT 0.455 MPa (printed specimens)70°Csourcecontinuous use operating range
Values forUltimaker ABS, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v5.00, April 20, 2022.Weir Minerals Linatex Premium rubber (95 % natural rubber), typical physical properties, spec sheet WMD0118/202305

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic ABS is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic ABS stronger than Rubber?

Plastic ABS is stronger: its yield strength is 38.1 MPa against tensile strength 23 MPa for Rubber (1.66x).

Which is lighter, Plastic ABS or Rubber?

Rubber is lighter: 960 kg/m³ against 1,100 kg/m³ for Plastic ABS.

Which is lighter for the same job, Plastic ABS or Rubber?

For the same stiffness or strength: Plastic ABS is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABSRubber
Strong rod or tielighter45% heavier
Strong beamlighter22% heavier
Strong panel or platelighter12% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic ABS or Rubber?

Rubber stretches further before it breaks: 830% elongation at break against 4.6% for Plastic ABS.

Which conducts heat better, Plastic ABS or Rubber?

Plastic ABS conducts heat better: 0.17 W/m·K against 0.151 W/m·K for Rubber.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABS
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABSRubber
Strength against density