Plastic ABS3D printed (FDM)
SLA Resin Standard3D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength38.1MPasourcetypicalnot given (tensile used)
Ultimate tensile strength38.1MPasourcetypical, peak stress (= stress at yield)60MPasourcetypical
Flexural strength61.1MPasourcetypical105MPasourcetypical1.72x stronger in bending
Elongation at break4.6%sourcetypical8%sourcetypical1.74x more ductile
Young's modulus (stiffness)1.96GPasourcetypical2.75GPasourcetypical40% stiffer
Density1,100kg/m³sourcetypicalnot sourced
Strength to weight34.6kN·m/kgnot sourced
Stiffness to weight1.78MN·m/kgnot sourced
Poisson's ratio0.39sourcebase material: ABS family typical (Covestro Part and Mold Design guide, Table 3-1)not sourced
Shear modulus0.706GPanot sourced
Bulk modulus2.97GPanot sourced
Speed of sound1,336m/snot sourced
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, typicalnot sourced
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, rangenot sourced
100 mm part over a 50 °C swing475µm growthnot sourced
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistance21.2W/mnot sourced
Glass transition101°Csourcetypicalnot sourced
Max service temperature86.6°CsourceHDT 0.455 MPa (printed specimens)59°CsourceHDT 1.8 MPa
Values forUltimaker ABS, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v5.00, April 20, 2022.Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic ABS and SLA Resin Standard are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic ABS stronger than SLA Resin Standard?

SLA Resin Standard is stronger: its tensile strength is 60 MPa against yield strength 38.1 MPa for Plastic ABS (1.57x).

Which is stiffer, Plastic ABS or SLA Resin Standard?

SLA Resin Standard is stiffer: Young's modulus 2.75 GPa against 1.96 GPa for Plastic ABS, so the same part in SLA Resin Standard deflects less under the same load.

Which is more ductile, Plastic ABS or SLA Resin Standard?

SLA Resin Standard stretches further before it breaks: 8% elongation at break against 4.6% for Plastic ABS.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABS
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABS