Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: UltiMaker, Cleveland-Cliffs, Covestro, Steel Construction Institute, INEOS Styrolution
Plastic ABS
Ultimaker ABS, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v5.00, April 20, 2022.
Stainless Steel 304
Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
304/304L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 304 · Yield strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Ultimate tensile strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Elongation at break: typical, annealed, in 2 in. (50.8 mm)Stainless Steel 304 · Young's modulus (stiffness): typical, in tensionStainless Steel 304 · Density: typicalStainless Steel 304 · Thermal conductivity: at 100 °CStainless Steel 304 · Thermal expansion: mean, 0–100 °CStainless Steel 304 · Specific heat: mean, 0–100 °CStainless Steel 304 · Melting point: melting rangeStainless Steel 304 · Max service temperature: continuous, oxidation (scaling) limit in air
3
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic ABS · Poisson's ratio: base material: ABS family typical (Covestro Part and Mold Design guide, Table 3-1)
4
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 304 · Poisson's ratio: design value (structural stainless steels)
5
Terluran GP-22 (ABS) Product Data SheetINEOS StyrolutionPlastic ABS · Thermal conductivity: base material: INEOS Styrolution Terluran GP-22 injection-molding ABS, typicalPlastic ABS · Thermal expansion: base material: INEOS Styrolution Terluran GP-22 injection-molding ABS, range
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Plastic ABS is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Plastic ABS stronger than Stainless Steel 304?
Stainless Steel 304 is stronger: its yield strength is 241 MPa against 38.1 MPa for Plastic ABS (6.33x).
Which is lighter, Plastic ABS or Stainless Steel 304?
Plastic ABS is lighter: 1,100 kg/m³ against 8,030 kg/m³ for Stainless Steel 304.
Which is stiffer, Plastic ABS or Stainless Steel 304?
Stainless Steel 304 is stiffer: Young's modulus 193 GPa against 1.96 GPa for Plastic ABS, so the same part in Stainless Steel 304 deflects less under the same load.
Which is lighter for the same job, Plastic ABS or Stainless Steel 304?
For the same stiffness or strength: Plastic ABS is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 304 is lighter for a stiff rod or tie (tension), stiff beam (bending).
Part that must be
Plastic ABS
Stainless Steel 304
Stiff rod or tie (tension)
13.5x heavier
lighter
Stiff beam (bending)
36% heavier
lighter
Stiff panel or plate
lighter
1.58x heavier
Strong rod or tie
lighter
15% heavier
Strong beam
lighter
2.13x heavier
Strong panel or plate
lighter
2.9x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic ABS or Stainless Steel 304?
Stainless Steel 304 stretches further before it breaks: 55% elongation at break against 4.6% for Plastic ABS.
Thermal
Which conducts heat better, Plastic ABS or Stainless Steel 304?
Stainless Steel 304 conducts heat better: 16.2 W/m·K against 0.17 W/m·K for Plastic ABS.
Which expands less with temperature?
Stainless Steel 304 expands less: 16.9 µm/m·K against 95 µm/m·K for Plastic ABS.