Materials / Compare

Plastic HDPE vs. SLA Resin Standard

Compare Plastic HDPE vs. SLA Resin Standard strength, stiffness, weight and thermal properties.

Change either side
Plastic HDPEBulk polymer (molded or machined)
SLA Resin Standard3D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength24MPasourcetypical, tensile stress at yield 23 °C, 50 mm/min ISO 527not given (tensile used)
Ultimate tensile strengthnot sourced60MPasourcetypical
Flexural strengthnot sourced105MPasourcetypical
Elongation at breaknot sourced8%sourcetypical
Young's modulus (stiffness)0.9GPasourcetypical, tensile modulus 23 °C ISO 5272.75GPasourcetypical
Density950kg/m³sourcetypical, ISO 1183not sourced
Strength to weight25.3kN·m/kgnot sourced
Stiffness to weight0.947MN·m/kgnot sourced
Poisson's ratio0.4–0.45sourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)not sourced
Shear modulus0.316GPanot sourced
Bulk modulus2GPanot sourced
Speed of sound973m/snot sourced
Thermal
Thermal conductivity0.4–0.49W/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)not sourced
Thermal expansion120µm/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)not sourced
100 mm part over a 50 °C swing600µm growthnot sourced
Specific heat2,250J/kg·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)not sourced
Heats up and cools (diffusivity)0.208mm²/snot sourced
Thermal shock resistance56.9W/mnot sourced
Max service temperaturenot sourced59°CsourceHDT 1.8 MPa
Values forLyondellBasell Hostalen 23050 B high density polyethylene, typical ISO valuesFormlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic HDPE stronger than SLA Resin Standard?

SLA Resin Standard is stronger: its tensile strength is 60 MPa against yield strength 24 MPa for Plastic HDPE (2.5x).

Which is stiffer, Plastic HDPE or SLA Resin Standard?

SLA Resin Standard is stiffer: Young's modulus 2.75 GPa against 0.9 GPa for Plastic HDPE, so the same part in SLA Resin Standard deflects less under the same load.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic HDPE
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic HDPE
Strength against density