Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: LyondellBasell, Cleveland-Cliffs, INEOS Olefins & Polymers USA
Plastic HDPE
LyondellBasell Hostalen 23050 B high density polyethylene, typical ISO values
Stainless Steel 17-4PH
Cleveland-Cliffs 17-4 PH, Condition H 900, sheet/strip, transverse (Product Data Bulletin, May 2021)
1
Hostalen 23050 B Product DataLyondellBasellPlastic HDPE · Yield strength: typical, tensile stress at yield 23 °C, 50 mm/min ISO 527Plastic HDPE · Young's modulus (stiffness): typical, tensile modulus 23 °C ISO 527Plastic HDPE · Density: typical, ISO 1183
2
17-4 PH Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 17-4PH · Yield strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Ultimate tensile strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Elongation at break: typical, transverse, in 2 in. (50.8 mm)Stainless Steel 17-4PH · Young's modulus (stiffness): H 900Stainless Steel 17-4PH · Density: H 900Stainless Steel 17-4PH · Poisson's ratio: H 900 (column)Stainless Steel 17-4PH · Thermal conductivity: at 149 °C (300 °F), H 900Stainless Steel 17-4PH · Thermal expansion: mean, 21–93 °C (70–200 °F), H 900Stainless Steel 17-4PH · Specific heat: mean, 0–100 °C, H 900Stainless Steel 17-4PH · Max service temperature: strength-retention limit (not oxidation)
3
Typical Engineering Properties of High Density PolyethyleneINEOS Olefins & Polymers USAarchived copyPlastic HDPE · Poisson's ratio: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal conductivity: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal expansion: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Specific heat: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic HDPE stronger than Stainless Steel 17-4PH?
Stainless Steel 17-4PH is stronger: its yield strength is 1,275 MPa against 24 MPa for Plastic HDPE (53.1x).
Which is lighter, Plastic HDPE or Stainless Steel 17-4PH?
Plastic HDPE is lighter: 950 kg/m³ against 7,800 kg/m³ for Stainless Steel 17-4PH.
Which is stiffer, Plastic HDPE or Stainless Steel 17-4PH?
Stainless Steel 17-4PH is stiffer: Young's modulus 197 GPa against 0.9 GPa for Plastic HDPE, so the same part in Stainless Steel 17-4PH deflects less under the same load.
Which is lighter for the same job, Plastic HDPE or Stainless Steel 17-4PH?
For the same stiffness or strength: Plastic HDPE is lighter for a stiff panel or plate, strong panel or plate; Stainless Steel 17-4PH is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam.
Part that must be
Plastic HDPE
Stainless Steel 17-4PH
Stiff rod or tie (tension)
26.7x heavier
lighter
Stiff beam (bending)
1.8x heavier
lighter
Stiff panel or plate
lighter
36% heavier
Strong rod or tie
6.47x heavier
lighter
Strong beam
1.72x heavier
lighter
Strong panel or plate
lighter
13% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Plastic HDPE or Stainless Steel 17-4PH?
Stainless Steel 17-4PH conducts heat better: 17.9 W/m·K against 0.445 W/m·K for Plastic HDPE.
Which expands less with temperature?
Stainless Steel 17-4PH expands less: 10.8 µm/m·K against 120 µm/m·K for Plastic HDPE.