Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: LyondellBasell, Cleveland-Cliffs, INEOS Olefins & Polymers USA, Steel Construction Institute
Plastic HDPE
LyondellBasell Hostalen 23050 B high density polyethylene, typical ISO values
Stainless Steel 304
Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
1
Hostalen 23050 B Product DataLyondellBasellPlastic HDPE · Yield strength: typical, tensile stress at yield 23 °C, 50 mm/min ISO 527Plastic HDPE · Young's modulus (stiffness): typical, tensile modulus 23 °C ISO 527Plastic HDPE · Density: typical, ISO 1183
2
304/304L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 304 · Yield strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Ultimate tensile strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Elongation at break: typical, annealed, in 2 in. (50.8 mm)Stainless Steel 304 · Young's modulus (stiffness): typical, in tensionStainless Steel 304 · Density: typicalStainless Steel 304 · Thermal conductivity: at 100 °CStainless Steel 304 · Thermal expansion: mean, 0–100 °CStainless Steel 304 · Specific heat: mean, 0–100 °CStainless Steel 304 · Melting point: melting rangeStainless Steel 304 · Max service temperature: continuous, oxidation (scaling) limit in air
3
Typical Engineering Properties of High Density PolyethyleneINEOS Olefins & Polymers USAarchived copyPlastic HDPE · Poisson's ratio: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal conductivity: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal expansion: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Specific heat: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
4
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 304 · Poisson's ratio: design value (structural stainless steels)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic HDPE stronger than Stainless Steel 304?
Stainless Steel 304 is stronger: its yield strength is 241 MPa against 24 MPa for Plastic HDPE (10x).
Which is lighter, Plastic HDPE or Stainless Steel 304?
Plastic HDPE is lighter: 950 kg/m³ against 8,030 kg/m³ for Stainless Steel 304.
Which is stiffer, Plastic HDPE or Stainless Steel 304?
Stainless Steel 304 is stiffer: Young's modulus 193 GPa against 0.9 GPa for Plastic HDPE, so the same part in Stainless Steel 304 deflects less under the same load.
Which is lighter for the same job, Plastic HDPE or Stainless Steel 304?
For the same stiffness or strength: Plastic HDPE is lighter for a stiff panel or plate, strong beam, strong panel or plate; Stainless Steel 304 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.
Part that must be
Plastic HDPE
Stainless Steel 304
Stiff rod or tie (tension)
25.4x heavier
lighter
Stiff beam (bending)
1.73x heavier
lighter
Stiff panel or plate
lighter
41% heavier
Strong rod or tie
19% heavier
lighter
Strong beam
lighter
1.82x heavier
Strong panel or plate
lighter
2.67x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Plastic HDPE or Stainless Steel 304?
Stainless Steel 304 conducts heat better: 16.2 W/m·K against 0.445 W/m·K for Plastic HDPE.
Which expands less with temperature?
Stainless Steel 304 expands less: 16.9 µm/m·K against 120 µm/m·K for Plastic HDPE.