Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources6 documents: LyondellBasell, American Institute of Steel Construction, bauforumstahl (ArcelorMittal), INEOS Olefins & Polymers USA, Ovako
Plastic HDPE
LyondellBasell Hostalen 23050 B high density polyethylene, typical ISO values
Steel
Generic structural steel, cited as ASTM A992 (the current US structural grade): ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
1
Hostalen 23050 B Product DataLyondellBasellPlastic HDPE · Yield strength: typical, tensile stress at yield 23 °C, 50 mm/min ISO 527Plastic HDPE · Young's modulus (stiffness): typical, tensile modulus 23 °C ISO 527Plastic HDPE · Density: typical, ISO 1183
2
Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
3
ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel · Young's modulus (stiffness): design value (AISC 360-16)Steel · Poisson's ratio: design value (AISC 360-16 Commentary)
4
Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel · Density: nominal (constructional data)Steel · Thermal conductivity: nominal at 20 °CSteel · Thermal expansion: nominal (constructional data, no temperature range stated)
5
Typical Engineering Properties of High Density PolyethyleneINEOS Olefins & Polymers USAarchived copyPlastic HDPE · Poisson's ratio: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal conductivity: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal expansion: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Specific heat: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
6
S275JR Steel GradeOvakoSteel · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic HDPE stronger than Steel?
Steel is stronger: its yield strength is 385 MPa against 24 MPa for Plastic HDPE (16x).
Which is lighter, Plastic HDPE or Steel?
Plastic HDPE is lighter: 950 kg/m³ against 7,850 kg/m³ for Steel.
Which is stiffer, Plastic HDPE or Steel?
Steel is stiffer: Young's modulus 200 GPa against 0.9 GPa for Plastic HDPE, so the same part in Steel deflects less under the same load.
Which is lighter for the same job, Plastic HDPE or Steel?
For the same stiffness or strength: Plastic HDPE is lighter for a stiff panel or plate, strong beam, strong panel or plate; Steel is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.
Part that must be
Plastic HDPE
Steel
Stiff rod or tie (tension)
26.9x heavier
lighter
Stiff beam (bending)
1.8x heavier
lighter
Stiff panel or plate
lighter
36% heavier
Strong rod or tie
1.94x heavier
lighter
Strong beam
lighter
30% heavier
Strong panel or plate
lighter
2.06x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Plastic HDPE or Steel?
Steel conducts heat better: 48 W/m·K against 0.445 W/m·K for Plastic HDPE.
Which expands less with temperature?
Steel expands less: 12 µm/m·K against 120 µm/m·K for Plastic HDPE.