Materials / Compare

Plastic Nylon PA6 vs. SLA Resin Standard

Compare Plastic Nylon PA6 vs. SLA Resin Standard strength, stiffness, weight and thermal properties.

Change either side
Plastic Nylon PA6Bulk polymer (molded or machined)
SLA Resin Standard3D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength90MPasourcetypical, drynot given (tensile used)
Ultimate tensile strengthnot sourced60MPasourcetypical
Flexural strengthnot sourced105MPasourcetypical
Elongation at break10%sourcenominal strain at break, dry8%sourcetypical
Young's modulus (stiffness)3.5GPasourcetypical, dry2.75GPasourcetypical
Density1,130kg/m³sourcetypicalnot sourced
Strength to weight79.6kN·m/kgnot sourced
Stiffness to weight3.1MN·m/kgnot sourced
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)not sourced
Shear modulus1.25GPanot sourced
Bulk modulus5.83GPanot sourced
Speed of sound1,760m/snot sourced
Thermal
Thermal conductivity0.33W/m·Ksourcetypicalnot sourced
Thermal expansion102µm/m·Ksourcelongitudinal, 23-55 °Cnot sourced
100 mm part over a 50 °C swing510µm growthnot sourced
Specific heat1,700J/kg·Ksourcetypicalnot sourced
Heats up and cools (diffusivity)0.172mm²/snot sourced
Thermal shock resistance49.9W/mnot sourced
Melting point220°CsourceDSCnot sourced
Max service temperature87°CsourceIEC 60216 temperature index, 20000 h59°CsourceHDT 1.8 MPa
Values forBASF Ultramid B3S (PA6, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic Nylon PA6 stronger than SLA Resin Standard?

Plastic Nylon PA6 is stronger: its yield strength is 90 MPa against tensile strength 60 MPa for SLA Resin Standard (1.5x).

Which is stiffer, Plastic Nylon PA6 or SLA Resin Standard?

Plastic Nylon PA6 is stiffer: Young's modulus 3.5 GPa against 2.75 GPa for SLA Resin Standard, so the same part in Plastic Nylon PA6 deflects less under the same load.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Nylon PA6
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic Nylon PA6
Strength against density

Related comparisons