Materials / Compare

Plastic Nylon PA6 vs. Stainless Steel 17-4PH

Compare Plastic Nylon PA6 vs. Stainless Steel 17-4PH strength, stiffness, weight and thermal properties.

Plastic Nylon PA6Bulk polymer (molded or machined)
Stainless Steel 17-4PHWrought
MechanicalPlastic Nylon PA6Stainless Steel 17-4PH
Yield strength90MPa11,275MPa214.2x stronger
Ultimate tensile strengthnot stated (yield given)1,379MPa2
Elongation at break10%19%2
Young's modulus (stiffness)3.5GPa1H 900197GPa256.3x stiffer
Density1,130kg/m³16.9x lighterH 9007,800kg/m³2
Strength to weight79.6kN·m/kg163kN·m/kg2.05x higher
Stiffness to weight3.1MN·m/kg25.3MN·m/kg8.15x higher
Poisson's ratiobase material0.43H 9000.2722
Shear modulus1.25GPa77.4GPa61.9x stiffer in shear
Bulk modulus5.83GPa144GPa24.7x higher
Speed of sound1,760m/s5,026m/s2.86x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Aluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon PA6Stainless Steel 17-4PH
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Aluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon PA6Stainless Steel 17-4PH
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic Nylon PA6Stainless Steel 17-4PH
Thermal conductivity0.33W/m·K1at 149 °C17.9W/m·K254.2x more heat through a fin
Thermal expansionlongitudinal102µm/m·K1mean10.8µm/m·K29.44x less
100 mm part over a 50 °C swing510µm growth54µm growth9.44x less
Specific heat1,700J/kg·K13.7x highermean460J/kg·K2
Heats up and cools (diffusivity)0.172mm²/s4.99mm²/s29x faster
Thermal shock resistance49.9W/m7,809W/m156x more resistant
Melting pointDSC220°C1not sourced
Max service temperature87°C1316°C2229 °C hotter
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Aluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon PA6Stainless Steel 17-4PH
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Aluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon PA6Stainless Steel 17-4PH
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: BASF, Cleveland-Cliffs, Covestro
Plastic Nylon PA6
BASF Ultramid B3S (PA6, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)
Stainless Steel 17-4PH
Cleveland-Cliffs 17-4 PH, Condition H 900, sheet/strip, transverse (Product Data Bulletin, May 2021)
  1. 1
    Ultramid B3S Product InformationBASFPlastic Nylon PA6 · Yield strength: typical, dryPlastic Nylon PA6 · Elongation at break: nominal strain at break, dryPlastic Nylon PA6 · Young's modulus (stiffness): typical, dryPlastic Nylon PA6 · Density: typicalPlastic Nylon PA6 · Thermal conductivity: typicalPlastic Nylon PA6 · Thermal expansion: longitudinal, 23-55 °CPlastic Nylon PA6 · Specific heat: typicalPlastic Nylon PA6 · Melting point: DSCPlastic Nylon PA6 · Max service temperature: IEC 60216 temperature index, 20000 h
  2. 2
    17-4 PH Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 17-4PH · Yield strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Ultimate tensile strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Elongation at break: typical, transverse, in 2 in. (50.8 mm)Stainless Steel 17-4PH · Young's modulus (stiffness): H 900Stainless Steel 17-4PH · Density: H 900Stainless Steel 17-4PH · Poisson's ratio: H 900 (column)Stainless Steel 17-4PH · Thermal conductivity: at 149 °C (300 °F), H 900Stainless Steel 17-4PH · Thermal expansion: mean, 21–93 °C (70–200 °F), H 900Stainless Steel 17-4PH · Specific heat: mean, 0–100 °C, H 900Stainless Steel 17-4PH · Max service temperature: strength-retention limit (not oxidation)
  3. 3
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon PA6 · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Plastic Nylon PA6 stronger than Stainless Steel 17-4PH?

Stainless Steel 17-4PH is stronger: its yield strength is 1,275 MPa against 90 MPa for Plastic Nylon PA6 (14.2x).

Which is lighter, Plastic Nylon PA6 or Stainless Steel 17-4PH?

Plastic Nylon PA6 is lighter: 1,130 kg/m³ against 7,800 kg/m³ for Stainless Steel 17-4PH.

Which is stiffer, Plastic Nylon PA6 or Stainless Steel 17-4PH?

Stainless Steel 17-4PH is stiffer: Young's modulus 197 GPa against 3.5 GPa for Plastic Nylon PA6, so the same part in Stainless Steel 17-4PH deflects less under the same load.

Which is lighter for the same job, Plastic Nylon PA6 or Stainless Steel 17-4PH?

For the same stiffness or strength: Plastic Nylon PA6 is lighter for a stiff panel or plate, strong beam, strong panel or plate; Stainless Steel 17-4PH is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.

Part that must bePlastic Nylon PA6Stainless Steel 17-4PH
Stiff rod or tie (tension)8.15x heavierlighter
Stiff beam (bending)9% heavierlighter
Stiff panel or platelighter1.8x heavier
Strong rod or tie2.05x heavierlighter
Strong beamlighter18% heavier
Strong panel or platelighter1.83x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which handles higher temperatures, Plastic Nylon PA6 or Stainless Steel 17-4PH?

Stainless Steel 17-4PH does: 316 °C against 87 °C for Plastic Nylon PA6.

Which conducts heat better, Plastic Nylon PA6 or Stainless Steel 17-4PH?

Stainless Steel 17-4PH conducts heat better: 17.9 W/m·K against 0.33 W/m·K for Plastic Nylon PA6.

Which expands less with temperature?

Stainless Steel 17-4PH expands less: 10.8 µm/m·K against 102 µm/m·K for Plastic Nylon PA6.

Related comparisons