Materials / Compare

Plastic Nylon vs. Steel A992

Compare Plastic Nylon vs. Steel A992 strength, stiffness, weight and thermal properties.

Plastic Nylon3D printed (FDM)
Steel A992Wrought
MechanicalPlastic NylonSteel A992
Yield strength63.1MPa1385MPa26.1x stronger
Ultimate tensile strength63.1MPa1505MPa28x stronger
Flexural strength82.9MPa1not sourced
Elongation at breaknot sourced24.2%2
Young's modulus (stiffness)2.33GPa1design value200GPa3
Density1,140kg/m³16.89x lighter7,850kg/m³4
Strength to weight55.4kN·m/kg13% higher49kN·m/kg
Stiffness to weight2.04MN·m/kg25.5MN·m/kg12.5x higher
Poisson's ratiobase material0.45design value0.33
Shear modulus0.833GPa76.9GPa92.4x stiffer in shear
Bulk modulus3.89GPa167GPa42.9x higher
Speed of sound1,430m/s5,048m/s3.53x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic NylonSteel A992
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPURubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic NylonSteel A992
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic NylonSteel A992
Thermal conductivitybase material0.33W/m·K648W/m·K4145x more heat through a fin
Thermal expansionbase material98–102µm/m·K612µm/m·K4
100 mm part over a 50 °C swing500µm growth60µm growth8.33x less
Specific heatbase material1,700J/kg·K6base material460–480J/kg·K7
Heats up and cools (diffusivity)0.17mm²/s13mm²/s76.4x faster
Thermal shock resistance53.6W/m5,390W/m101x more resistant
Melting point188°C1not sourced
Glass transition55.1°C1not sourced
Max service temperatureHDT 0.455 MPa89.2°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic NylonSteel A992
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic NylonSteel A992
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources7 documents: UltiMaker, American Institute of Steel Construction, bauforumstahl (ArcelorMittal), Covestro, BASF, Ovako
Plastic Nylon
Ultimaker Nylon, 3D-printed specimens, XY (flat), conditioned >=24 h at room temperature; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v2.00, April 20, 2022.
Steel A992
ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
  1. 1
    Ultimaker Nylon Technical Data Sheet, v5.00UltiMakerarchived copyPlastic Nylon · Yield strength: typicalPlastic Nylon · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic Nylon · Flexural strength: typicalPlastic Nylon · Young's modulus (stiffness): typicalPlastic Nylon · Density: typicalPlastic Nylon · Melting point: typicalPlastic Nylon · Glass transition: typicalPlastic Nylon · Max service temperature: HDT 0.455 MPa (printed specimens)
  2. 2
    Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel A992 · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel A992 · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel A992 · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
  3. 3
    ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel A992 · Young's modulus (stiffness): design value (AISC 360-16)Steel A992 · Poisson's ratio: design value (AISC 360-16 Commentary)
  4. 4
    Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel A992 · Density: nominal (constructional data)Steel A992 · Thermal conductivity: nominal at 20 °CSteel A992 · Thermal expansion: nominal (constructional data, no temperature range stated)
  5. 5
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
  6. 6
    Ultramid (PA) Product RangeBASFPlastic Nylon · Thermal conductivity: base material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)Plastic Nylon · Thermal expansion: base material: unreinforced BASF Ultramid PA66 (A3K, 98) and PA6 (B3S, 102), 23-55 CPlastic Nylon · Specific heat: base material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)
  7. 7
    S275JR Steel GradeOvakoSteel A992 · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Plastic Nylon stronger than Steel A992?

Steel A992 is stronger: its yield strength is 385 MPa against 63.1 MPa for Plastic Nylon (6.1x).

Which is lighter, Plastic Nylon or Steel A992?

Plastic Nylon is lighter: 1,140 kg/m³ against 7,850 kg/m³ for Steel A992.

Which is stiffer, Plastic Nylon or Steel A992?

Steel A992 is stiffer: Young's modulus 200 GPa against 2.33 GPa for Plastic Nylon, so the same part in Steel A992 deflects less under the same load.

Which is lighter for the same job, Plastic Nylon or Steel A992?

For the same stiffness or strength: Plastic Nylon is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Steel A992 is lighter for a stiff rod or tie (tension), stiff beam (bending).

Part that must bePlastic NylonSteel A992
Stiff rod or tie (tension)12.5x heavierlighter
Stiff beam (bending)35% heavierlighter
Stiff panel or platelighter1.56x heavier
Strong rod or tielighter13% heavier
Strong beamlighter2.06x heavier
Strong panel or platelighter2.79x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Plastic Nylon or Steel A992?

Steel A992 conducts heat better: 48 W/m·K against 0.33 W/m·K for Plastic Nylon.

Which expands less with temperature?

Steel A992 expands less: 12 µm/m·K against 100 µm/m·K for Plastic Nylon.

Related comparisons