Plastic PBT GF30Bulk polymer (molded or machined)
Plastic PMMABulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength140MPasourcestress at break, 23 °C80MPasourcetypical, 23 °C
Compressive strengthnot sourced110MPasourcecompressive yield stress, typical
Flexural strength210MPasourcetypical, 23 °C115MPasourcetypical
Elongation at break3%sourcestrain at break, 23 °C5.5%sourcetypical
Young's modulus (stiffness)9.8GPasourcetypical, 23 °C3.3GPasourcetypical, short-term
Density1,530kg/m³sourcetypical1,190kg/m³sourcetypical29% lighter
Strength to weight91.5kN·m/kg36% higher67.2kN·m/kg
Stiffness to weight6.41MN·m/kg2.31x higher2.77MN·m/kg
Poisson's rationot sourced0.37sourcetypical
Shear modulusnot sourced1.2GPa
Bulk modulusnot sourced4.23GPa
Speed of sound2,531m/s1,665m/s
Thermal
Thermal conductivity0.27W/m·Ksourcetypical (DIN 52612-1)0.19W/m·Ksourcetypical
Thermal expansion25µm/m·Ksourcelongitudinal (flow), mean 23-55 °C70µm/m·Ksource0-50 °C
100 mm part over a 50 °C swing125µm growth2.8x less350µm growth
Specific heat1,050J/kg·Ksourcetypical, 23 °C1,470J/kg·Ksourcetypical
Heats up and cools (diffusivity)0.168mm²/s1.55x faster0.109mm²/s
Thermal shock resistancenot sourced41.5W/m
Melting point223°CsourceDSC (ISO 11357)not sourced
Max service temperature205°CsourceHDT 1.8 MPa80°Csourcemax. permanent service temperature
Values forBASF Ultradur B 4300 G6 (PBT, 30% glass fibre), injection moulding grade; product information sheet 09/2026, typical values for uncoloured product at 23 °C.Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic PBT GF30 stronger than Plastic PMMA?

Plastic PBT GF30 is stronger: its tensile strength is 140 MPa against 80 MPa for Plastic PMMA (1.75x).

Which is lighter, Plastic PBT GF30 or Plastic PMMA?

Plastic PMMA is lighter: 1,190 kg/m³ against 1,530 kg/m³ for Plastic PBT GF30.

Which is stiffer, Plastic PBT GF30 or Plastic PMMA?

Plastic PBT GF30 is stiffer: Young's modulus 9.8 GPa against 3.3 GPa for Plastic PMMA, so the same part in Plastic PBT GF30 deflects less under the same load.

Which is lighter for the same job, Plastic PBT GF30 or Plastic PMMA?

For the same stiffness or strength: Plastic PBT GF30 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PBT GF30Plastic PMMA
Stiff rod or tie (tension)lighter2.31x heavier
Stiff beam (bending)lighter34% heavier
Stiff panel or platelighter12% heavier
Strong rod or tielighter36% heavier
Strong beamlighter13% heavier
Strong panel or platelighter3% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic PBT GF30 or Plastic PMMA?

Plastic PBT GF30 conducts heat better: 0.27 W/m·K against 0.19 W/m·K for Plastic PMMA.

Which expands less with temperature?

Plastic PBT GF30 expands less: 25 µm/m·K against 70 µm/m·K for Plastic PMMA.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PPS GF40Plastic LCP GF30Plastic PBT GF30Plastic PMMA
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PPS GF40Plastic LCP GF30Plastic PBT GF30Plastic PMMA
Strength against density