Materials / Compare

Plastic PETG vs. Plastic PLA

Compare Plastic PETG vs. Plastic PLA strength, stiffness, weight and thermal properties.

Change either side
Plastic PETG3D printed (FDM)
Plastic PLA3D printed (FDM)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength46.2MPasourcetypical52.5MPasourcetypical14% stronger
Ultimate tensile strength46.2MPasourcetypical, peak stress (= stress at yield)52.5MPasourcetypical, peak stress (= stress at yield)14% stronger
Flexural strength78.9MPasourcetypical96.8MPasourcetypical23% stronger in bending
Elongation at break7.6%sourcetypical7.8%sourcetypical
Young's modulus (stiffness)1.94GPasourcetypical3.25GPasourcetypical1.68x stiffer
Density1,270kg/m³sourcetypical1,240kg/m³sourcetypical
Strength to weight36.4kN·m/kg42.3kN·m/kg16% higher
Stiffness to weight1.53MN·m/kg2.62MN·m/kg1.72x higher
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound1,236m/s1,619m/s
Thermal
Thermal conductivity0.21W/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical0.13W/m·Ksourcebase material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C
Thermal expansion51µm/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typicalnot sourced
100 mm part over a 50 °C swing255µm growthnot sourced
Specific heat1,300J/kg·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)1,200J/kg·Ksourcebase material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C
Heats up and cools (diffusivity)0.127mm²/s46% faster0.0874mm²/s
Thermal shock resistancenot sourcednot sourced
Melting pointnot sourced152°Csourcetypical
Glass transition77.4°Csourcetypical59.1°Csourcetypical
Max service temperature76.2°CsourceHDT 0.455 MPa (printed specimens)30% hotter58.8°CsourceHDT 0.455 MPa (printed specimens)
Values forUltimaker PETG, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v1.00, April 29, 2022.Ultimaker PLA, 3D-printed specimens, XY (flat) orientation; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS dated April 20, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PETG and Plastic PLA are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic PETG stronger than Plastic PLA?

Plastic PLA is stronger: its yield strength is 52.5 MPa against 46.2 MPa for Plastic PETG (14%).

Which is lighter, Plastic PETG or Plastic PLA?

Plastic PLA is lighter: 1,240 kg/m³ against 1,270 kg/m³ for Plastic PETG.

Which is stiffer, Plastic PETG or Plastic PLA?

Plastic PLA is stiffer: Young's modulus 3.25 GPa against 1.94 GPa for Plastic PETG, so the same part in Plastic PLA deflects less under the same load.

Which is lighter for the same job, Plastic PETG or Plastic PLA?

For the same stiffness or strength: Plastic PLA is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PETGPlastic PLA
Stiff rod or tie (tension)1.72x heavierlighter
Stiff beam (bending)33% heavierlighter
Stiff panel or plate22% heavierlighter
Strong rod or tie16% heavierlighter
Strong beam12% heavierlighter
Strong panel or plate9% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which handles higher temperatures, Plastic PETG or Plastic PLA?

Plastic PETG does: 76.2 °C against 58.8 °C for Plastic PLA, both HDT 0.455 MPa (printed specimens).

Which conducts heat better, Plastic PETG or Plastic PLA?

Plastic PETG conducts heat better: 0.21 W/m·K against 0.13 W/m·K for Plastic PLA.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PETGPlastic PLA
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PETGPlastic PLA
Strength against density