Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
TIMETAL 6-4 PropertiesTIMETarchived copyTitanium Ti-6Al-4V · Yield strength: typical, plate (>0.187 in), annealed, 0.2% offsetTitanium Ti-6Al-4V · Ultimate tensile strength: typical, plate, annealedTitanium Ti-6Al-4V · Elongation at break: typical, in 2 in., plate annealedTitanium Ti-6Al-4V · Density: nominalTitanium Ti-6Al-4V · Poisson's ratio: mean of TIMET measurementsTitanium Ti-6Al-4V · Melting point: melting rangeTitanium Ti-6Al-4V · Max service temperature: upper recommended use temperature
3
TIMETAL 6-4 Data SheetTIMETarchived copyTitanium Ti-6Al-4V · Young's modulus (stiffness): typical range, 20 °CTitanium Ti-6Al-4V · Thermal conductivity: typical, 20 °C, mill annealedTitanium Ti-6Al-4V · Thermal expansion: typical, mean 0-100 °CTitanium Ti-6Al-4V · Specific heat: typical, 20 °C
4
Eastar Copolyester 6763 Product Data SheetEastmanPlastic PETG · Thermal conductivity: base material: Eastman Eastar Copolyester 6763 (PETG), typicalPlastic PETG · Thermal expansion: base material: Eastman Eastar Copolyester 6763 (PETG), typicalPlastic PETG · Specific heat: base material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Plastic PETG is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Plastic PETG stronger than Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V is stronger: its yield strength is 885 MPa against 46.2 MPa for Plastic PETG (19.2x).
Which is lighter, Plastic PETG or Titanium Ti-6Al-4V?
Plastic PETG is lighter: 1,270 kg/m³ against 4,430 kg/m³ for Titanium Ti-6Al-4V.
Which is stiffer, Plastic PETG or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V is stiffer: Young's modulus 115 GPa against 1.94 GPa for Plastic PETG, so the same part in Titanium Ti-6Al-4V deflects less under the same load.
Which is lighter for the same job, Plastic PETG or Titanium Ti-6Al-4V?
For the same stiffness or strength: Titanium Ti-6Al-4V is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Plastic PETG
Titanium Ti-6Al-4V
Stiff rod or tie (tension)
16.9x heavier
lighter
Stiff beam (bending)
2.2x heavier
lighter
Stiff panel or plate
12% heavier
lighter
Strong rod or tie
5.49x heavier
lighter
Strong beam
2.05x heavier
lighter
Strong panel or plate
25% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PETG or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V stretches further before it breaks: 16% elongation at break against 7.6% for Plastic PETG.
Thermal
Which conducts heat better, Plastic PETG or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V conducts heat better: 6.6 W/m·K against 0.21 W/m·K for Plastic PETG.
Which expands less with temperature?
Titanium Ti-6Al-4V expands less: 9 µm/m·K against 51 µm/m·K for Plastic PETG.