Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: American Institute of Steel Construction, Röhm, bauforumstahl (ArcelorMittal), Ovako
Plastic PMMA
Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)
Steel
Generic structural steel, cited as ASTM A992 (the current US structural grade): ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
1
Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
2
PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1)Röhmarchived copyPlastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature
3
ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel · Young's modulus (stiffness): design value (AISC 360-16)Steel · Poisson's ratio: design value (AISC 360-16 Commentary)
4
Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel · Density: nominal (constructional data)Steel · Thermal conductivity: nominal at 20 °CSteel · Thermal expansion: nominal (constructional data, no temperature range stated)
5
S275JR Steel GradeOvakoSteel · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic PMMA stronger than Steel?
Steel is stronger: its yield strength is 385 MPa against tensile strength 80 MPa for Plastic PMMA (4.81x).
Which is lighter, Plastic PMMA or Steel?
Plastic PMMA is lighter: 1,190 kg/m³ against 7,850 kg/m³ for Steel.
Which is stiffer, Plastic PMMA or Steel?
Steel is stiffer: Young's modulus 200 GPa against 3.3 GPa for Plastic PMMA, so the same part in Steel deflects less under the same load.
Which is lighter for the same job, Plastic PMMA or Steel?
For the same stiffness or strength: Plastic PMMA is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Steel is lighter for a stiff rod or tie (tension), stiff beam (bending).
Part that must be
Plastic PMMA
Steel
Stiff rod or tie (tension)
9.19x heavier
lighter
Stiff beam (bending)
18% heavier
lighter
Stiff panel or plate
lighter
1.68x heavier
Strong rod or tie
lighter
37% heavier
Strong beam
lighter
2.31x heavier
Strong panel or plate
lighter
3.01x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PMMA or Steel?
Steel stretches further before it breaks: 24.2% elongation at break against 5.5% for Plastic PMMA.
Thermal
Which conducts heat better, Plastic PMMA or Steel?
Steel conducts heat better: 48 W/m·K against 0.19 W/m·K for Plastic PMMA.
Which expands less with temperature?
Steel expands less: 12 µm/m·K against 70 µm/m·K for Plastic PMMA.