Materials / Compare

Plastic POM/Acetal vs. Zinc Zamak 3

Compare Plastic POM/Acetal vs. Zinc Zamak 3 strength, stiffness, weight and thermal properties.

Plastic POM/AcetalBulk polymer (molded or machined)
Zinc Zamak 3Cast
MechanicalPlastic POM/AcetalZinc Zamak 3
Yield strength69MPa1221MPa23.2x stronger
Ultimate tensile strength69MPa1283MPa24.1x stronger
Compressive strength124MPa1not sourced
Flexural strength99MPa1not sourced
Elongation at break75%17.5x more ductile10%2
Young's modulus (stiffness)2.8GPa185.5GPa230.5x stiffer
Density1,420kg/m³34.65x lighter6,600kg/m³2
Strength to weight48.6kN·m/kg45% higher33.5kN·m/kg
Stiffness to weight1.97MN·m/kg13MN·m/kg6.57x higher
Poisson's ratio0.3510.274
Shear modulus1.04GPa33.7GPa32.5x stiffer in shear
Bulk modulus3.11GPa62GPa19.9x higher
Speed of sound1,404m/s3,599m/s2.56x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic POM/AcetalZinc Zamak 3
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic POM/AcetalZinc Zamak 3
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic POM/AcetalZinc Zamak 3
Thermal conductivity0.4W/m·K1113W/m·K2283x more heat through a fin
Thermal expansionmean122µm/m·K127.4µm/m·K24.45x less
100 mm part over a 50 °C swing610µm growth137µm growth4.45x less
Specific heataverage -18 to 100 °C1,465J/kg·K13.5x higher419J/kg·K2
Heats up and cools (diffusivity)0.192mm²/s40.9mm²/s213x faster
Thermal shock resistance52.5W/m7,782W/m148x more resistant
Melting point175°C1melting range381–387°C2
Max service temperatureHDT 1.8 MPa125°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic POM/AcetalZinc Zamak 3
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic POM/AcetalZinc Zamak 3
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: DuPont, Nathan Trotter, Eastern Alloys
Plastic POM/Acetal
DuPont Delrin 100 acetal homopolymer, Table 2 'Typical Properties of Delrin Acetal Resins' (ASTM methods), Delrin Design Guide Module III hosted on delrin.com
Zinc Zamak 3
Zamak 3 (ASTM B86 die cast), Nathan Trotter (zinc alloy producer) technical data sheet, typical values
  1. 1
    Delrin Acetal Resin Design Guide, Module IIIDuPontarchived copyPlastic POM/Acetal · Yield strength: typical (single ASTM D638 tensile strength)Plastic POM/Acetal · Ultimate tensile strength: typicalPlastic POM/Acetal · Compressive strength: compressive stress at 10% deformationPlastic POM/Acetal · Flexural strength: flexural yield strength, typicalPlastic POM/Acetal · Elongation at break: typicalPlastic POM/Acetal · Young's modulus (stiffness): typicalPlastic POM/Acetal · Poisson's ratio: typicalPlastic POM/Acetal · Thermal conductivity: typicalPlastic POM/Acetal · Thermal expansion: mean, 29 to 60 °CPlastic POM/Acetal · Specific heat: average -18 to 100 °C, Delrin acetal resins (not grade-specific)Plastic POM/Acetal · Melting point: crystalline melting pointPlastic POM/Acetal · Max service temperature: HDT 1.8 MPa (annealed)
  2. 2
    Zamak 3 Technical Data SheetNathan Trotterarchived copyZinc Zamak 3 · Yield strength: typicalZinc Zamak 3 · Ultimate tensile strength: typicalZinc Zamak 3 · Elongation at break: typical, in 2 in.Zinc Zamak 3 · Young's modulus (stiffness): typicalZinc Zamak 3 · Density: typicalZinc Zamak 3 · Thermal conductivity: typicalZinc Zamak 3 · Thermal expansion: typicalZinc Zamak 3 · Specific heat: typicalZinc Zamak 3 · Melting point: melting range
  3. 3
    Delrin 100 Product Data SheetDuPontPlastic POM/Acetal · Density: typical (DuPont product information for Delrin 100 NC010; 'The data listed here fall within the normal range of product properties')
  4. 4
    Zinc Die Casting Properties Guide (2012)Eastern AlloysZinc Zamak 3 · Poisson's ratio: typical, Zamak 3 hot-chamber die cast

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Plastic POM/Acetal stronger than Zinc Zamak 3?

Zinc Zamak 3 is stronger: its yield strength is 221 MPa against 69 MPa for Plastic POM/Acetal (3.2x).

Which is lighter, Plastic POM/Acetal or Zinc Zamak 3?

Plastic POM/Acetal is lighter: 1,420 kg/m³ against 6,600 kg/m³ for Zinc Zamak 3.

Which is stiffer, Plastic POM/Acetal or Zinc Zamak 3?

Zinc Zamak 3 is stiffer: Young's modulus 85.5 GPa against 2.8 GPa for Plastic POM/Acetal, so the same part in Zinc Zamak 3 deflects less under the same load.

Which is lighter for the same job, Plastic POM/Acetal or Zinc Zamak 3?

For the same stiffness or strength: Plastic POM/Acetal is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Zinc Zamak 3 is lighter for a stiff rod or tie (tension), stiff beam (bending).

Part that must bePlastic POM/AcetalZinc Zamak 3
Stiff rod or tie (tension)6.57x heavierlighter
Stiff beam (bending)19% heavierlighter
Stiff panel or platelighter49% heavier
Strong rod or tielighter45% heavier
Strong beamlighter2.14x heavier
Strong panel or platelighter2.6x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic POM/Acetal or Zinc Zamak 3?

Plastic POM/Acetal stretches further before it breaks: 75% elongation at break against 10% for Zinc Zamak 3.

Thermal

Which conducts heat better, Plastic POM/Acetal or Zinc Zamak 3?

Zinc Zamak 3 conducts heat better: 113 W/m·K against 0.4 W/m·K for Plastic POM/Acetal.

Which expands less with temperature?

Zinc Zamak 3 expands less: 27.4 µm/m·K against 122 µm/m·K for Plastic POM/Acetal.

Related comparisons