Materials / Compare

Plastic PPS GF40 vs. Steel A992

Compare Plastic PPS GF40 vs. Steel A992 strength, stiffness, weight and thermal properties.

Change either side
Plastic PPS GF40Bulk polymer (molded or machined)
Steel A992Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)385MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISC
Ultimate tensile strength195MPasourcetensile strength, 5 mm/min505MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)
Flexural strength285MPasourceflexural strength at breaknot sourced
Elongation at break1.9%sourcestrain at break, 5 mm/minnot sourced
Young's modulus (stiffness)14.7GPasourcetypical, 1 mm/min200GPasourcedesign value (AISC 360-16)
Density1,650kg/m³sourcetypical7,850kg/m³sourcenominal (constructional data)
Strength to weight118kN·m/kg2.41x higher49kN·m/kg
Stiffness to weight8.91MN·m/kg25.5MN·m/kg2.86x higher
Poisson's ratio0.35sourceglass-reinforced Fortron PPS (class value, not grade-specific)0.3sourcedesign value (AISC 360-16 Commentary)
Shear modulus5.44GPa76.9GPa14.1x stiffer in shear
Bulk modulus16.3GPa167GPa
Speed of sound2,985m/s5,048m/s
Thermal
Thermal conductivity0.2W/m·Ksource40% glass-reinforced Fortron, 25 °C (not grade-specific)48W/m·Ksourcenominal at 20 °C
Thermal expansion12µm/m·Ksourceparallel (flow), mean -50 to 90 °C12µm/m·Ksourcenominal (constructional data, no temperature range stated)
100 mm part over a 50 °C swing60µm growth60µm growth
Specific heatnot sourced460–480J/kg·Ksourcebase material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Heats up and cools (diffusivity)not sourced13mm²/s
Thermal shock resistance144W/m5,390W/m37.5x more resistant
Melting point280°CsourceDSC, 10 °C/minnot sourced
Glass transition90°CsourceDSC, 10 °C/minnot sourced
Max service temperature270°CsourceHDT 1.8 MPanot sourced
Values forCelanese Fortron 1140L4 (PPS, 40% glass fibre), injection moulding; FORTRON PPS Short-Term Properties Guide (PPS-012, 2016); thermal conductivity and Poisson for 40% glass-reinforced Fortron from the Fortron PPS Design Manual (PPS-050, 2013).ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic PPS GF40 stronger than Steel A992?

Steel A992 is stronger: its yield strength is 385 MPa against tensile strength 195 MPa for Plastic PPS GF40 (1.97x).

Which is lighter, Plastic PPS GF40 or Steel A992?

Plastic PPS GF40 is lighter: 1,650 kg/m³ against 7,850 kg/m³ for Steel A992.

Which is stiffer, Plastic PPS GF40 or Steel A992?

Steel A992 is stiffer: Young's modulus 200 GPa against 14.7 GPa for Plastic PPS GF40, so the same part in Steel A992 deflects less under the same load.

Which is lighter for the same job, Plastic PPS GF40 or Steel A992?

For the same stiffness or strength: Plastic PPS GF40 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Steel A992 is lighter for a stiff rod or tie (tension).

Part that must bePlastic PPS GF40Steel A992
Stiff rod or tie (tension)2.86x heavierlighter
Stiff beam (bending)lighter29% heavier
Stiff panel or platelighter1.99x heavier
Strong rod or tielighter2.41x heavier
Strong beamlighter3.02x heavier
Strong panel or platelighter3.39x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic PPS GF40 or Steel A992?

Steel A992 conducts heat better: 48 W/m·K against 0.2 W/m·K for Plastic PPS GF40.

Which expands less with temperature?

Plastic PPS GF40 expands less: 12 µm/m·K against 12 µm/m·K for Steel A992.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic LCP GF30Plastic PPS GF40Steel A992
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic LCP GF30Plastic PPS GF40Steel A992
Strength against density

Related comparisons