Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: ATI, Formlabs, Steel Construction Institute
SLA Resin Elastic 50A
Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.
Stainless Steel 316
ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
1
ATI 316, 316L, 317 and 317L Technical Data Sheet (2012)ATIarchived copyStainless Steel 316 · Yield strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Ultimate tensile strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Elongation at break: typical (representative), annealed, in 2 in. (51 mm)Stainless Steel 316 · Young's modulus (stiffness): typical, in tensionStainless Steel 316 · Density: typicalStainless Steel 316 · Thermal conductivity: 20–100 °CStainless Steel 316 · Thermal expansion: mean, 20–100 °CStainless Steel 316 · Specific heat: at 20 °CStainless Steel 316 · Melting point: melting rangeStainless Steel 316 · Max service temperature: oxidation (scaling) limit in air
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 316 · Poisson's ratio: design value (structural stainless steels)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is SLA Resin Elastic 50A stronger than Stainless Steel 316?
Stainless Steel 316 is stronger: its yield strength is 265 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (77.9x).
Which is lighter, SLA Resin Elastic 50A or Stainless Steel 316?
SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 8,027 kg/m³ for Stainless Steel 316.
Which is lighter for the same job, SLA Resin Elastic 50A or Stainless Steel 316?
For the same stiffness or strength: Stainless Steel 316 is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
SLA Resin Elastic 50A
Stainless Steel 316
Strong rod or tie
9.81x heavier
lighter
Strong beam
2.3x heavier
lighter
Strong panel or plate
11% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, SLA Resin Elastic 50A or Stainless Steel 316?
SLA Resin Elastic 50A stretches further before it breaks: 160% elongation at break against 61% for Stainless Steel 316.