Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.
Stainless Steel 17-4PH
Cleveland-Cliffs 17-4 PH, Condition H 900, sheet/strip, transverse (Product Data Bulletin, May 2021)
1
17-4 PH Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 17-4PH · Yield strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Ultimate tensile strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Elongation at break: typical, transverse, in 2 in. (50.8 mm)Stainless Steel 17-4PH · Young's modulus (stiffness): H 900Stainless Steel 17-4PH · Density: H 900Stainless Steel 17-4PH · Poisson's ratio: H 900 (column)Stainless Steel 17-4PH · Thermal conductivity: at 149 °C (300 °F), H 900Stainless Steel 17-4PH · Thermal expansion: mean, 21–93 °C (70–200 °F), H 900Stainless Steel 17-4PH · Specific heat: mean, 0–100 °C, H 900Stainless Steel 17-4PH · Max service temperature: strength-retention limit (not oxidation)
2
Clear Resin V5 Technical Data Sheet (2024)Formlabsarchived copySLA Resin Standard · Ultimate tensile strength: typicalSLA Resin Standard · Flexural strength: typicalSLA Resin Standard · Elongation at break: typicalSLA Resin Standard · Young's modulus (stiffness): typicalSLA Resin Standard · Max service temperature: HDT 1.8 MPa
3
Clear Resin V5 Technical Data Sheet (web edition)FormlabsSLA Resin Standard · Density: typical, post-cured (same for 5 min ambient and 15 min at 60 °C), ASTM D792
4
Thermal Properties of Selected Formlabs SLA ResinsFormlabsSLA Resin Standard · Thermal conductivity: typical, post-cured, ASTM E1530SLA Resin Standard · Thermal expansion: mean -30 to 140 °C, post-cured (5 min ambient cure), TMA ASTM E831SLA Resin Standard · Specific heat: typical, 25 °C, post-cured (5 min ambient cure), DSC ASTM E1269
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is SLA Resin Standard stronger than Stainless Steel 17-4PH?
Stainless Steel 17-4PH is stronger: its yield strength is 1,275 MPa against tensile strength 60 MPa for SLA Resin Standard (21.3x).
Which is lighter, SLA Resin Standard or Stainless Steel 17-4PH?
SLA Resin Standard is lighter: 1,210 kg/m³ against 7,800 kg/m³ for Stainless Steel 17-4PH.
Which is stiffer, SLA Resin Standard or Stainless Steel 17-4PH?
Stainless Steel 17-4PH is stiffer: Young's modulus 197 GPa against 2.75 GPa for SLA Resin Standard, so the same part in Stainless Steel 17-4PH deflects less under the same load.
Which is lighter for the same job, SLA Resin Standard or Stainless Steel 17-4PH?
For the same stiffness or strength: SLA Resin Standard is lighter for a stiff panel or plate, strong panel or plate; Stainless Steel 17-4PH is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam.
Part that must be
SLA Resin Standard
Stainless Steel 17-4PH
Stiff rod or tie (tension)
11.1x heavier
lighter
Stiff beam (bending)
31% heavier
lighter
Stiff panel or plate
lighter
1.55x heavier
Strong rod or tie
3.3x heavier
lighter
Strong beam
19% heavier
lighter
Strong panel or plate
lighter
40% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, SLA Resin Standard or Stainless Steel 17-4PH?
Stainless Steel 17-4PH stretches further before it breaks: 9% elongation at break against 8% for SLA Resin Standard.
Thermal
Which conducts heat better, SLA Resin Standard or Stainless Steel 17-4PH?
Stainless Steel 17-4PH conducts heat better: 17.9 W/m·K against 0.54 W/m·K for SLA Resin Standard.
Which expands less with temperature?
Stainless Steel 17-4PH expands less: 10.8 µm/m·K against 114 µm/m·K for SLA Resin Standard.