Stainless Steel 17-4PHWrought
Stainless Steel 316Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength1,275MPasourcetypical, transverse, sheet/strip265MPasourcetypical (representative), annealed 1.0 mm sheet
Ultimate tensile strength1,379MPasourcetypical, transverse, sheet/strip583MPasourcetypical (representative), annealed 1.0 mm sheet
Elongation at break9%sourcetypical, transverse, in 2 in. (50.8 mm)61%sourcetypical (representative), annealed, in 2 in. (51 mm)
Young's modulus (stiffness)197GPasourceH 900200GPasourcetypical, in tension
Density7,800kg/m³sourceH 9008,027kg/m³sourcetypical
Strength to weight163kN·m/kg4.95x higher33kN·m/kg
Stiffness to weight25.3MN·m/kg1% higher24.9MN·m/kg
Poisson's ratio0.272sourceH 900 (column)0.3sourcedesign value (structural stainless steels)
Shear modulus77.4GPa76.9GPa
Bulk modulus144GPa167GPa
Speed of sound5,026m/s4,992m/s
Thermal
Thermal conductivity17.9W/m·Ksourceat 149 °C (300 °F), H 90014.6W/m·Ksource20–100 °C
Thermal expansion10.8µm/m·Ksourcemean, 21–93 °C (70–200 °F), H 90016.5µm/m·Ksourcemean, 20–100 °C
100 mm part over a 50 °C swing54µm growth1.53x less82.5µm growth
Specific heat460J/kg·Ksourcemean, 0–100 °C, H 900450J/kg·Ksourceat 20 °C
Heats up and cools (diffusivity)4.99mm²/s23% faster4.04mm²/s
Thermal shock resistance7,809W/m9.52x more resistant821W/m
Melting pointnot sourced1,390–1,440°Csourcemelting range
Max service temperature316°Csourcestrength-retention limit (not oxidation)871–899°Csourceoxidation (scaling) limit in air
Values forCleveland-Cliffs 17-4 PH, Condition H 900, sheet/strip, transverse (Product Data Bulletin, May 2021)ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Stainless Steel 17-4PH stronger than Stainless Steel 316?

Stainless Steel 17-4PH is stronger: its yield strength is 1,275 MPa against 265 MPa for Stainless Steel 316 (4.81x).

Which is lighter, Stainless Steel 17-4PH or Stainless Steel 316?

Stainless Steel 17-4PH is lighter: 7,800 kg/m³ against 8,027 kg/m³ for Stainless Steel 316.

Which is stiffer, Stainless Steel 17-4PH or Stainless Steel 316?

Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 197 GPa for Stainless Steel 17-4PH, so the same part in Stainless Steel 316 deflects less under the same load.

Which is lighter for the same job, Stainless Steel 17-4PH or Stainless Steel 316?

For the same stiffness or strength: Stainless Steel 17-4PH is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beStainless Steel 17-4PHStainless Steel 316
Stiff rod or tie (tension)lighter1% heavier
Stiff beam (bending)lighter2% heavier
Stiff panel or platelighter2% heavier
Strong rod or tielighter4.95x heavier
Strong beamlighter2.93x heavier
Strong panel or platelighter2.26x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Stainless Steel 17-4PH or Stainless Steel 316?

Stainless Steel 17-4PH conducts heat better: 17.9 W/m·K against 14.6 W/m·K for Stainless Steel 316.

Which expands less with temperature?

Stainless Steel 17-4PH expands less: 10.8 µm/m·K against 16.5 µm/m·K for Stainless Steel 316.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Aluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Stainless Steel 17-4PHStainless Steel 316
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Aluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Stainless Steel 17-4PHStainless Steel 316
Strength against density

Related comparisons