Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Cleveland-Cliffs, American Institute of Steel Construction, bauforumstahl (ArcelorMittal), Ovako
Stainless Steel 17-4PH
Cleveland-Cliffs 17-4 PH, Condition H 900, sheet/strip, transverse (Product Data Bulletin, May 2021)
Steel
Generic structural steel, cited as ASTM A992 (the current US structural grade): ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
1
17-4 PH Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 17-4PH · Yield strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Ultimate tensile strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Elongation at break: typical, transverse, in 2 in. (50.8 mm)Stainless Steel 17-4PH · Young's modulus (stiffness): H 900Stainless Steel 17-4PH · Density: H 900Stainless Steel 17-4PH · Poisson's ratio: H 900 (column)Stainless Steel 17-4PH · Thermal conductivity: at 149 °C (300 °F), H 900Stainless Steel 17-4PH · Thermal expansion: mean, 21–93 °C (70–200 °F), H 900Stainless Steel 17-4PH · Specific heat: mean, 0–100 °C, H 900Stainless Steel 17-4PH · Max service temperature: strength-retention limit (not oxidation)
2
Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
3
ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel · Young's modulus (stiffness): design value (AISC 360-16)Steel · Poisson's ratio: design value (AISC 360-16 Commentary)
4
Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel · Density: nominal (constructional data)Steel · Thermal conductivity: nominal at 20 °CSteel · Thermal expansion: nominal (constructional data, no temperature range stated)
5
S275JR Steel GradeOvakoSteel · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Stainless Steel 17-4PH stronger than Steel?
Stainless Steel 17-4PH is stronger: its yield strength is 1,275 MPa against 385 MPa for Steel (3.31x).
Which is lighter, Stainless Steel 17-4PH or Steel?
Stainless Steel 17-4PH is lighter: 7,800 kg/m³ against 7,850 kg/m³ for Steel.
Which is stiffer, Stainless Steel 17-4PH or Steel?
Steel is stiffer: Young's modulus 200 GPa against 197 GPa for Stainless Steel 17-4PH, so the same part in Steel deflects less under the same load.
Which is lighter for the same job, Stainless Steel 17-4PH or Steel?
For the same stiffness or strength: Stainless Steel 17-4PH is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Stainless Steel 17-4PH
Steel
Stiff rod or tie (tension)
about equal
about equal
Stiff beam (bending)
about equal
about equal
Stiff panel or plate
about equal
about equal
Strong rod or tie
lighter
3.33x heavier
Strong beam
lighter
2.24x heavier
Strong panel or plate
lighter
1.83x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Stainless Steel 17-4PH or Steel?
Steel stretches further before it breaks: 24.2% elongation at break against 9% for Stainless Steel 17-4PH.
Thermal
Which conducts heat better, Stainless Steel 17-4PH or Steel?
Steel conducts heat better: 48 W/m·K against 17.9 W/m·K for Stainless Steel 17-4PH.
Which expands less with temperature?
Stainless Steel 17-4PH expands less: 10.8 µm/m·K against 12 µm/m·K for Steel.