Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Kaiser Aluminum, Victrex, U.S. Department of Defense
Aluminum 6061-T6
6061-T6/T651, Kaiser Aluminum typical properties; Poisson from MIL-HDBK-5J
Plastic PEEK
Victrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)
1
Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 6061-T6 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 6061-T6 · Ultimate tensile strength: typicalAluminum 6061-T6 · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum 6061-T6 · Young's modulus (stiffness): typicalAluminum 6061-T6 · Density: nominalAluminum 6061-T6 · Thermal conductivity: typical, 20 °CAluminum 6061-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 6061-T6 · Specific heat: typical, at 100 °CAluminum 6061-T6 · Melting point: solidus-liquidus
2
VICTREX PEEK 450G Technical Data SheetVictrexPlastic PEEK · Yield strength: typical, tensile yieldPlastic PEEK · Compressive strength: typical, 23 CPlastic PEEK · Flexural strength: typical, flexural stress at yield, 23 CPlastic PEEK · Elongation at break: typical, at breakPlastic PEEK · Young's modulus (stiffness): typical (nominal)Plastic PEEK · Density: typical (crystalline)Plastic PEEK · Thermal conductivity: typical, average, 23 CPlastic PEEK · Thermal expansion: average of flow/cross-flow, below Tg (<143 C)Plastic PEEK · Melting point: typical, DSCPlastic PEEK · Glass transition: onset (midpoint 150 C)Plastic PEEK · Max service temperature: UL 746B RTI, mechanical strength (continuous use index)
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 6061-T6 · Poisson's ratio: typical (handbook physical constant)
4
VICTREX PEEK for Use in Fluid Management (2020)VictrexPlastic PEEK · Poisson's ratio: typical
5
VICTREX PEEK 450G Technical Data Sheet (2012)Victrexarchived copyPlastic PEEK · Specific heat: typical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 6061-T6 stronger than Plastic PEEK?
Aluminum 6061-T6 is stronger: its yield strength is 276 MPa against 98 MPa for Plastic PEEK (2.82x).
Which is lighter, Aluminum 6061-T6 or Plastic PEEK?
Plastic PEEK is lighter: 1,300 kg/m³ against 2,700 kg/m³ for Aluminum 6061-T6.
Which is stiffer, Aluminum 6061-T6 or Plastic PEEK?
Aluminum 6061-T6 is stiffer: Young's modulus 68.3 GPa against 4 GPa for Plastic PEEK, so the same part in Aluminum 6061-T6 deflects less under the same load.
Which is lighter for the same job, Aluminum 6061-T6 or Plastic PEEK?
For the same stiffness or strength: Aluminum 6061-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie; Plastic PEEK is lighter for a strong beam, strong panel or plate.
Part that must be
Aluminum 6061-T6
Plastic PEEK
Stiff rod or tie (tension)
lighter
8.22x heavier
Stiff beam (bending)
lighter
1.99x heavier
Stiff panel or plate
lighter
24% heavier
Strong rod or tie
lighter
36% heavier
Strong beam
4% heavier
lighter
Strong panel or plate
24% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 6061-T6 or Plastic PEEK?
Plastic PEEK stretches further before it breaks: 25% elongation at break against 17% for Aluminum 6061-T6.
Thermal
Which conducts heat better, Aluminum 6061-T6 or Plastic PEEK?
Aluminum 6061-T6 conducts heat better: 167 W/m·K against 0.29 W/m·K for Plastic PEEK.
Which expands less with temperature?
Aluminum 6061-T6 expands less: 23.6 µm/m·K against 55 µm/m·K for Plastic PEEK.