Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Ultimaker PC Technical Data Sheet, v5.00UltiMakerarchived copyFDM Polycarbonate · Yield strength: typicalFDM Polycarbonate · Ultimate tensile strength: typical, peak stress (= stress at yield)FDM Polycarbonate · Flexural strength: typicalFDM Polycarbonate · Elongation at break: typicalFDM Polycarbonate · Young's modulus (stiffness): typicalFDM Polycarbonate · Density: rangeFDM Polycarbonate · Glass transition: typicalFDM Polycarbonate · Max service temperature: HDT 0.455 MPa (printed specimens)
3
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyFDM Polycarbonate · Poisson's ratio: base material: polycarbonate family typical (Covestro Part and Mold Design guide, Table 3-1)
4
Makrolon 2405 Technical Data SheetCovestroFDM Polycarbonate · Thermal conductivity: base material: Covestro Makrolon 2405 injection-molding PC, typical, through-plane, 23 °CFDM Polycarbonate · Thermal expansion: base material: Covestro Makrolon 2405 injection-molding PC, typical, 23-55 °C, parallel
5
Technical Datasheet, Extruded Products: Alloy EN AW-6063 (Rev. 4, 2023)Hydroarchived copyAluminum 6063-T6 · Specific heat: typical, 20 °C (Hydro EN AW-6063)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM Polycarbonate is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 6063-T6 stronger than FDM Polycarbonate?
Aluminum 6063-T6 is stronger: its yield strength is 215 MPa against 53.3 MPa for FDM Polycarbonate (4.03x).
Which is lighter, Aluminum 6063-T6 or FDM Polycarbonate?
FDM Polycarbonate is lighter: 1,190 kg/m³ against 2,700 kg/m³ for Aluminum 6063-T6.
Which is stiffer, Aluminum 6063-T6 or FDM Polycarbonate?
Aluminum 6063-T6 is stiffer: Young's modulus 69 GPa against 2.39 GPa for FDM Polycarbonate, so the same part in Aluminum 6063-T6 deflects less under the same load.
Which is lighter for the same job, Aluminum 6063-T6 or FDM Polycarbonate?
For the same stiffness or strength: Aluminum 6063-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam; FDM Polycarbonate is lighter for a strong panel or plate.
Part that must be
Aluminum 6063-T6
FDM Polycarbonate
Stiff rod or tie (tension)
lighter
12.7x heavier
Stiff beam (bending)
lighter
2.37x heavier
Stiff panel or plate
lighter
35% heavier
Strong rod or tie
lighter
1.78x heavier
Strong beam
lighter
12% heavier
Strong panel or plate
13% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 6063-T6 or FDM Polycarbonate?
Aluminum 6063-T6 stretches further before it breaks: 12% elongation at break against 9.2% for FDM Polycarbonate.
Thermal
Which conducts heat better, Aluminum 6063-T6 or FDM Polycarbonate?
Aluminum 6063-T6 conducts heat better: 201 W/m·K against 0.2 W/m·K for FDM Polycarbonate.
Which expands less with temperature?
Aluminum 6063-T6 expands less: 23.4 µm/m·K against 65 µm/m·K for FDM Polycarbonate.