Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Sources9 documents: Kaiser Aluminum, National Ready Mixed Concrete Association, Federal Highway Administration, U.S. Department of Defense, Oak Ridge National Laboratory, USDA Forest Products Laboratory, National Institute of Standards and Technology
Aluminum 7050-T7451
7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J
Concrete
Normal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC review
CIP 36: Structural Lightweight ConcreteNational Ready Mixed Concrete Associationarchived copyConcrete · Density: range for normalweight concrete
5
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7050-T7451 · Poisson's ratio: typical (handbook physical constant)
6
The Effect of Elevated Temperature on Concrete Materials and Structures: A Literature Review (ORNL/TM-2005/553)Oak Ridge National Laboratoryarchived copyConcrete · Poisson's ratio: general range at normal ambient conditions (overall 0.11-0.32)Concrete · Max service temperature: code long-term temperature limit (ASME Code, concrete containments)
Thermal Coefficient of Portland Cement ConcreteFederal Highway AdministrationConcrete · Thermal expansion: typical range for portland cement concrete (aggregate dependent)
9
Best Practice Guidelines for Structural Fire Resistance Design of Concrete and Steel Buildings (TN 1681)National Institute of Standards and Technologyarchived copyConcrete · Specific heat: typical (NIST guidance for thermal analysis)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Which is lighter, Aluminum 7050-T7451 or Concrete?
Concrete is lighter: 2,320 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.
Which is stiffer, Aluminum 7050-T7451 or Concrete?
Aluminum 7050-T7451 is stiffer: Young's modulus 70.3 GPa against 25.1 GPa for Concrete, so the same part in Aluminum 7050-T7451 deflects less under the same load.
Which is lighter for the same job, Aluminum 7050-T7451 or Concrete?
For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.
Part that must be
Aluminum 7050-T7451
Concrete
Stiff rod or tie (tension)
lighter
2.3x heavier
Stiff beam (bending)
lighter
37% heavier
Stiff panel or plate
lighter
16% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Aluminum 7050-T7451 or Concrete?
Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 0.9 W/m·K for Concrete.
Which expands less with temperature?
Concrete expands less: 10 µm/m·K against 23.5 µm/m·K for Aluminum 7050-T7451.