Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Makrolon 2405 Technical Data SheetCovestroPlastic Polycarbonate · Yield strength: typical, tensile yieldPlastic Polycarbonate · Ultimate tensile strength: typical, stress at breakPlastic Polycarbonate · Flexural strength: typical, flexural strengthPlastic Polycarbonate · Elongation at break: typical, strain at breakPlastic Polycarbonate · Young's modulus (stiffness): typicalPlastic Polycarbonate · Density: typicalPlastic Polycarbonate · Thermal conductivity: typical, through-plane, 23 CPlastic Polycarbonate · Thermal expansion: typical, 23-55 C, parallel and normalPlastic Polycarbonate · Glass transition: typical, DSC 10 C/minPlastic Polycarbonate · Max service temperature: UL 746B RTI, tensile strength, 1.5 mm
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7050-T7451 · Poisson's ratio: typical (handbook physical constant)
4
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic Polycarbonate · Poisson's ratio: typical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
5
Makrolon 2405 Data Sheet, ASTM valuesBayer MaterialSciencearchived copyPlastic Polycarbonate · Specific heat: typical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 7050-T7451 stronger than Plastic Polycarbonate?
Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against 65 MPa for Plastic Polycarbonate (7.22x).
Which is lighter, Aluminum 7050-T7451 or Plastic Polycarbonate?
Plastic Polycarbonate is lighter: 1,200 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.
Which is stiffer, Aluminum 7050-T7451 or Plastic Polycarbonate?
Aluminum 7050-T7451 is stiffer: Young's modulus 70.3 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Aluminum 7050-T7451 deflects less under the same load.
Which is lighter for the same job, Aluminum 7050-T7451 or Plastic Polycarbonate?
For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 7050-T7451
Plastic Polycarbonate
Stiff rod or tie (tension)
lighter
12.4x heavier
Stiff beam (bending)
lighter
2.29x heavier
Stiff panel or plate
lighter
31% heavier
Strong rod or tie
lighter
3.06x heavier
Strong beam
lighter
1.58x heavier
Strong panel or plate
lighter
14% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 7050-T7451 or Plastic Polycarbonate?
Plastic Polycarbonate stretches further before it breaks: 125% elongation at break against 11% for Aluminum 7050-T7451.
Thermal
Which conducts heat better, Aluminum 7050-T7451 or Plastic Polycarbonate?
Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.
Which expands less with temperature?
Aluminum 7050-T7451 expands less: 23.5 µm/m·K against 65 µm/m·K for Plastic Polycarbonate.