Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Ultimaker PC Technical Data Sheet, v5.00UltiMakerarchived copyFDM Polycarbonate · Yield strength: typicalFDM Polycarbonate · Ultimate tensile strength: typical, peak stress (= stress at yield)FDM Polycarbonate · Flexural strength: typicalFDM Polycarbonate · Elongation at break: typicalFDM Polycarbonate · Young's modulus (stiffness): typicalFDM Polycarbonate · Density: rangeFDM Polycarbonate · Glass transition: typicalFDM Polycarbonate · Max service temperature: HDT 0.455 MPa (printed specimens)
3
Wieland-Z30 (CuZn39Pb2, C37700) Data SheetWielandarchived copyBrass C360 · Poisson's ratio: base material: leaded free-machining brass CuZn39Pb2 (C37700), Wieland-Z30 rolled products, reference value at room temperature
4
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyFDM Polycarbonate · Poisson's ratio: base material: polycarbonate family typical (Covestro Part and Mold Design guide, Table 3-1)
5
Makrolon 2405 Technical Data SheetCovestroFDM Polycarbonate · Thermal conductivity: base material: Covestro Makrolon 2405 injection-molding PC, typical, through-plane, 23 °CFDM Polycarbonate · Thermal expansion: base material: Covestro Makrolon 2405 injection-molding PC, typical, 23-55 °C, parallel
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM Polycarbonate is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Brass C360 stronger than FDM Polycarbonate?
Brass C360 is stronger: its yield strength is 310 MPa against 53.3 MPa for FDM Polycarbonate (5.82x).
Which is lighter, Brass C360 or FDM Polycarbonate?
FDM Polycarbonate is lighter: 1,190 kg/m³ against 8,498 kg/m³ for Brass C360.
Which is stiffer, Brass C360 or FDM Polycarbonate?
Brass C360 is stiffer: Young's modulus 96.5 GPa against 2.39 GPa for FDM Polycarbonate, so the same part in Brass C360 deflects less under the same load.
Which is lighter for the same job, Brass C360 or FDM Polycarbonate?
For the same stiffness or strength: Brass C360 is lighter for a stiff rod or tie (tension); FDM Polycarbonate is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Brass C360
FDM Polycarbonate
Stiff rod or tie (tension)
lighter
5.64x heavier
Stiff beam (bending)
12% heavier
lighter
Stiff panel or plate
2.08x heavier
lighter
Strong rod or tie
23% heavier
lighter
Strong beam
2.21x heavier
lighter
Strong panel or plate
2.96x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Brass C360 or FDM Polycarbonate?
Brass C360 stretches further before it breaks: 25% elongation at break against 9.2% for FDM Polycarbonate.
Thermal
Which conducts heat better, Brass C360 or FDM Polycarbonate?
Brass C360 conducts heat better: 116 W/m·K against 0.2 W/m·K for FDM Polycarbonate.
Which expands less with temperature?
Brass C360 expands less: 20.5 µm/m·K against 65 µm/m·K for FDM Polycarbonate.