Materials / Compare

Brick vs. Plastic Nylon

Compare Brick vs. Plastic Nylon strength, stiffness, weight and thermal properties.

BrickNatural
Plastic Nylon3D printed (FDM)
MechanicalBrickPlastic Nylon
Yield strengthnone (brittle)63.1MPa1
Ultimate tensile strengthmodulus of rupture5.1MPa263.1MPa1
Compressive strength77.9MPa3not sourced
Flexural strengthnot sourced82.9MPa1
Elongation at breaknone (brittle)not sourced
Young's modulus (stiffness)not sourced2.33GPa1
Density2,082kg/m³41,140kg/m³11.83x lighter
Strength to weight2.45kN·m/kg55.4kN·m/kg22.6x higher
Stiffness to weightnot sourced2.04MN·m/kg
Poisson's rationot sourcedbase material0.45
Shear modulusnot sourced0.833GPa
Bulk modulusnot sourced3.89GPa
Speed of soundnot sourced1,430m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPURubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30BrickPlastic Nylon
Strength against densityHigher and further left: stronger for its weight
ThermalBrickPlastic Nylon
Thermal conductivity0.92–1.12W/m·K4base material0.33W/m·K6
Thermal expansion7.2µm/m·K3base material98–102µm/m·K6
100 mm part over a 50 °C swing36µm growth13.9x less500µm growth
Specific heat837J/kg·K7base material1,700J/kg·K62.03x higher
Heats up and cools (diffusivity)0.585mm²/s3.44x faster0.17mm²/s
Thermal shock resistancenot sourced53.6W/m
Melting pointnot sourced188°C1
Glass transitionnot sourced55.1°C1
Max service temperaturenot sourcedHDT 0.455 MPa89.2°C1
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30BrickPlastic Nylon
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30BrickPlastic Nylon
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources7 documents: UltiMaker, National Institute of Standards and Technology, Brick Industry Association, Covestro, BASF
Brick
Solid extruded clay/shale brick units (BIA 1993 manufacturer survey, TN 3A 2024); face brick of 130 lb/ft3 for thermal properties (BIA TN 4, from ASHRAE 2013); CTE is the TMS Code value for clay/shale masonry
Plastic Nylon
Ultimaker Nylon, 3D-printed specimens, XY (flat), conditioned >=24 h at room temperature; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v2.00, April 20, 2022.
  1. 1
    Ultimaker Nylon Technical Data Sheet, v5.00UltiMakerarchived copyPlastic Nylon · Yield strength: typicalPlastic Nylon · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic Nylon · Flexural strength: typicalPlastic Nylon · Young's modulus (stiffness): typicalPlastic Nylon · Density: typicalPlastic Nylon · Melting point: typicalPlastic Nylon · Glass transition: typicalPlastic Nylon · Max service temperature: HDT 0.455 MPa (printed specimens)
  2. 2
    Strength of Masonry Walls Under Compressive and Transverse Loads (Building Science Series 34)National Institute of Standards and Technologyarchived copyBrick · Ultimate tensile strength: modulus of rupture (no direct tensile value)
  3. 3
    Technical Notes 3A: Brick Masonry Material PropertiesBrick Industry AssociationBrick · Compressive strength: mean unit compressive strength, solid extruded brick (survey mean; SD 30.8 MPa)Brick · Thermal expansion: TMS Code average coefficient, clay/shale unit masonry
  4. 4
    Technical Notes 4: Introduction to Energy Performance of Brick Masonry (2016)Brick Industry Associationarchived copyBrick · Density: face brick density row used for k (BIA notes most fired clay brick 120-130 lb/ft3)Brick · Thermal conductivity: range for 130 lb/ft3 face brick (ASHRAE 2013 via BIA)
  5. 5
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
  6. 6
    Ultramid (PA) Product RangeBASFPlastic Nylon · Thermal conductivity: base material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)Plastic Nylon · Thermal expansion: base material: unreinforced BASF Ultramid PA66 (A3K, 98) and PA6 (B3S, 102), 23-55 CPlastic Nylon · Specific heat: base material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)
  7. 7
    Technical Notes 4B: Energy Code Compliance of Brick Masonry WallsBrick Industry Associationarchived copyBrick · Specific heat: value used in BIA heat-capacity sample calculation

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Brick stronger than Plastic Nylon?

Plastic Nylon is stronger: its yield strength is 63.1 MPa against tensile strength 5.1 MPa for Brick (12.4x).

Which is lighter, Brick or Plastic Nylon?

Plastic Nylon is lighter: 1,140 kg/m³ against 2,082 kg/m³ for Brick.

Which is lighter for the same job, Brick or Plastic Nylon?

For the same stiffness or strength: Plastic Nylon is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beBrickPlastic Nylon
Strong rod or tie22.6x heavierlighter
Strong beam9.77x heavierlighter
Strong panel or plate6.42x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Brick or Plastic Nylon?

Brick conducts heat better: 1.02 W/m·K against 0.33 W/m·K for Plastic Nylon.

Which expands less with temperature?

Brick expands less: 7.2 µm/m·K against 100 µm/m·K for Plastic Nylon.