MechanicalCopper C110Nickel Inconel 718
Yield strength69MPa11,207MPa217.5x stronger
Ultimate tensile strength221MPa11,389MPa26.29x stronger
Elongation at break55%12.75x more ductile20%2
Young's modulus (stiffness)117GPa1200GPa21.71x stiffer
Density8,913kg/m³18,221kg/m³2
Strength to weight7.74kN·m/kg147kN·m/kg19x higher
Stiffness to weight13.1MN·m/kg24.3MN·m/kg1.85x higher
Poisson's ratio0.3430.2942
Shear modulus43.7GPa77.3GPa1.77x stiffer in shear
Bulk modulus122GPa162GPa33% higher
Speed of sound3,626m/s4,932m/s36% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Nickel Inconel 718
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Nickel Inconel 718
Strength against densityHigher and further left: stronger for its weight
ThermalCopper C110Nickel Inconel 718
Thermal conductivity391W/m·K134.3x more heat through a fin11.4W/m·K2
Thermal expansion16.9µm/m·K113.2µm/m·K228% less
100 mm part over a 50 °C swing84.5µm growth66µm growth28% less
Specific heat385J/kg·K1435J/kg·K213% higher
Heats up and cools (diffusivity)114mm²/s35.7x faster3.19mm²/s
Thermal shock resistance8,992W/m2.44x more resistant3,680W/m
Melting pointsolidus-liquidus1,065–1,083°C1melting range1,260–1,336°C2
Max service temperaturenot sourced704°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Nickel Inconel 718
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Nickel Inconel 718
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Copper Development Association, Special Metals, Wieland
Copper C110
C11000 ETP copper, annealed to 0.050 mm grain size (OS050), 1 in. rod, copper.org typical values
Nickel Inconel 718
INCONEL alloy 718, standard grade, 1750 °F/1 hr anneal + 1325 °F/8 hr F.C. to 1150 °F aged; Special Metals bulletin SMC-045 typical values
  1. 1
    C11000 Alloy (copper.org)Copper Development Associationarchived copyCopper C110 · Yield strength: typical, 0.5% extension under loadCopper C110 · Ultimate tensile strength: typicalCopper C110 · Elongation at break: typical, 1 in. rodCopper C110 · Young's modulus (stiffness): typicalCopper C110 · Density: nominalCopper C110 · Thermal conductivity: typical, 20 °CCopper C110 · Thermal expansion: typical, mean 20-100 °CCopper C110 · Specific heat: typical, 20 °CCopper C110 · Melting point: solidus-liquidus
  2. 2
    INCONEL alloy 718 (SMC-045)Special Metalsarchived copyNickel Inconel 718 · Yield strength: typical, 1.0 in. hot-rolled bar, 0.2% offsetNickel Inconel 718 · Ultimate tensile strength: typical, 1.0 in. barNickel Inconel 718 · Elongation at break: typical, 1.0 in. barNickel Inconel 718 · Young's modulus (stiffness): typical, 21 °C, annealed + agedNickel Inconel 718 · Density: nominal, annealed and agedNickel Inconel 718 · Poisson's ratio: typical, 21 °C, annealed + agedNickel Inconel 718 · Thermal conductivity: typical, 21 °C, annealed + aged (calculated from resistivity per footnote a)Nickel Inconel 718 · Thermal expansion: typical, mean 21-93 °C, annealed + agedNickel Inconel 718 · Specific heat: typical, 21 °CNickel Inconel 718 · Melting point: melting rangeNickel Inconel 718 · Max service temperature: upper use temperature stated by producer
  3. 3
    Wieland-K32 (Cu-ETP, C11000) Data SheetWielandarchived copyCopper C110 · Poisson's ratio: reference value at room temperature (Wieland-K32 = Cu-ETP = C11000, rolled products)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Copper C110 stronger than Nickel Inconel 718?

Nickel Inconel 718 is stronger: its yield strength is 1,207 MPa against 69 MPa for Copper C110 (17.5x).

Which is lighter, Copper C110 or Nickel Inconel 718?

Nickel Inconel 718 is lighter: 8,221 kg/m³ against 8,913 kg/m³ for Copper C110.

Which is stiffer, Copper C110 or Nickel Inconel 718?

Nickel Inconel 718 is stiffer: Young's modulus 200 GPa against 117 GPa for Copper C110, so the same part in Nickel Inconel 718 deflects less under the same load.

Which is lighter for the same job, Copper C110 or Nickel Inconel 718?

For the same stiffness or strength: Nickel Inconel 718 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beCopper C110Nickel Inconel 718
Stiff rod or tie (tension)1.85x heavierlighter
Stiff beam (bending)42% heavierlighter
Stiff panel or plate30% heavierlighter
Strong rod or tie19x heavierlighter
Strong beam7.31x heavierlighter
Strong panel or plate4.53x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Copper C110 or Nickel Inconel 718?

Copper C110 stretches further before it breaks: 55% elongation at break against 20% for Nickel Inconel 718.

Thermal

Which conducts heat better, Copper C110 or Nickel Inconel 718?

Copper C110 conducts heat better: 391 W/m·K against 11.4 W/m·K for Nickel Inconel 718.

Which expands less with temperature?

Nickel Inconel 718 expands less: 13.2 µm/m·K against 16.9 µm/m·K for Copper C110.