Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources6 documents: EOS GmbH, BASF, Renishaw, U.S. Department of Defense, Covestro
DMLS AlSi10Mg Aluminum
EOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10
Plastic Nylon PA6
BASF Ultramid B3S (PA6, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)
1
EOS Aluminium AlSi10Mg Material Data SheetEOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Yield strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Ultimate tensile strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Elongation at break: typical at break, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Thermal conductivity: typical, as manufactured, horizontal (ISO 22007-2)DMLS AlSi10Mg Aluminum · Thermal expansion: mean 25-100 °C, ASTM E228
RenAM 500 Series Aluminium AlSi10Mg Material Data SheetRenishawDMLS AlSi10Mg Aluminum · Young's modulus (stiffness): same material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY)
4
EOS Aluminium AlSi10Mg Material Data Sheet, FlexLine, M 290 (2018)EOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Density: typical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm)
5
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseDMLS AlSi10Mg Aluminum · Poisson's ratio: base material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000)DMLS AlSi10Mg Aluminum · Specific heat: base material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C
6
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon PA6 · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS AlSi10Mg Aluminum is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS AlSi10Mg Aluminum stronger than Plastic Nylon PA6?
DMLS AlSi10Mg Aluminum is stronger: its yield strength is 270 MPa against 90 MPa for Plastic Nylon PA6 (3x).
Which is lighter, DMLS AlSi10Mg Aluminum or Plastic Nylon PA6?
Plastic Nylon PA6 is lighter: 1,130 kg/m³ against 2,670 kg/m³ for DMLS AlSi10Mg Aluminum.
Which is stiffer, DMLS AlSi10Mg Aluminum or Plastic Nylon PA6?
DMLS AlSi10Mg Aluminum is stiffer: Young's modulus 72 GPa against 3.5 GPa for Plastic Nylon PA6, so the same part in DMLS AlSi10Mg Aluminum deflects less under the same load.
Which is lighter for the same job, DMLS AlSi10Mg Aluminum or Plastic Nylon PA6?
For the same stiffness or strength: DMLS AlSi10Mg Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie; Plastic Nylon PA6 is lighter for a strong beam, strong panel or plate.
Part that must be
DMLS AlSi10Mg Aluminum
Plastic Nylon PA6
Stiff rod or tie (tension)
lighter
8.71x heavier
Stiff beam (bending)
lighter
1.92x heavier
Stiff panel or plate
lighter
16% heavier
Strong rod or tie
lighter
27% heavier
Strong beam
14% heavier
lighter
Strong panel or plate
36% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, DMLS AlSi10Mg Aluminum or Plastic Nylon PA6?
DMLS AlSi10Mg Aluminum conducts heat better: 110 W/m·K against 0.33 W/m·K for Plastic Nylon PA6.
Which expands less with temperature?
DMLS AlSi10Mg Aluminum expands less: 20 µm/m·K against 102 µm/m·K for Plastic Nylon PA6.