Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources8 documents: EOS GmbH, American Institute of Steel Construction, Renishaw, bauforumstahl (ArcelorMittal), U.S. Department of Defense, Ovako
DMLS AlSi10Mg Aluminum
EOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10
Steel
Generic structural steel, cited as ASTM A992 (the current US structural grade): ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
1
EOS Aluminium AlSi10Mg Material Data SheetEOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Yield strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Ultimate tensile strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Elongation at break: typical at break, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Thermal conductivity: typical, as manufactured, horizontal (ISO 22007-2)DMLS AlSi10Mg Aluminum · Thermal expansion: mean 25-100 °C, ASTM E228
2
Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
3
RenAM 500 Series Aluminium AlSi10Mg Material Data SheetRenishawDMLS AlSi10Mg Aluminum · Young's modulus (stiffness): same material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY)
4
ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel · Young's modulus (stiffness): design value (AISC 360-16)Steel · Poisson's ratio: design value (AISC 360-16 Commentary)
5
EOS Aluminium AlSi10Mg Material Data Sheet, FlexLine, M 290 (2018)EOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Density: typical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm)
6
Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel · Density: nominal (constructional data)Steel · Thermal conductivity: nominal at 20 °CSteel · Thermal expansion: nominal (constructional data, no temperature range stated)
7
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseDMLS AlSi10Mg Aluminum · Poisson's ratio: base material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000)DMLS AlSi10Mg Aluminum · Specific heat: base material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C
8
S275JR Steel GradeOvakoSteel · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS AlSi10Mg Aluminum is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS AlSi10Mg Aluminum stronger than Steel?
Steel is stronger: its yield strength is 385 MPa against 270 MPa for DMLS AlSi10Mg Aluminum (43%).
Which is lighter, DMLS AlSi10Mg Aluminum or Steel?
DMLS AlSi10Mg Aluminum is lighter: 2,670 kg/m³ against 7,850 kg/m³ for Steel.
Which is stiffer, DMLS AlSi10Mg Aluminum or Steel?
Steel is stiffer: Young's modulus 200 GPa against 72 GPa for DMLS AlSi10Mg Aluminum, so the same part in Steel deflects less under the same load.
Which is lighter for the same job, DMLS AlSi10Mg Aluminum or Steel?
For the same stiffness or strength: DMLS AlSi10Mg Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
DMLS AlSi10Mg Aluminum
Steel
Stiff rod or tie (tension)
lighter
6% heavier
Stiff beam (bending)
lighter
1.76x heavier
Stiff panel or plate
lighter
2.09x heavier
Strong rod or tie
lighter
2.06x heavier
Strong beam
lighter
2.32x heavier
Strong panel or plate
lighter
2.46x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, DMLS AlSi10Mg Aluminum or Steel?
Steel stretches further before it breaks: 24.2% elongation at break against 10.2% for DMLS AlSi10Mg Aluminum.
Thermal
Which conducts heat better, DMLS AlSi10Mg Aluminum or Steel?
DMLS AlSi10Mg Aluminum conducts heat better: 110 W/m·K against 48 W/m·K for Steel.
Which expands less with temperature?
Steel expands less: 12 µm/m·K against 20 µm/m·K for DMLS AlSi10Mg Aluminum.