Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources6 documents: EOS GmbH, Niagara LaSalle, Renishaw, Ovako, U.S. Department of Defense
DMLS AlSi10Mg Aluminum
EOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10
Steel AISI 1045
AISI 1045 cold drawn bar (Niagara LaSalle) for mechanical; Ovako C45 (lists 'SAE 1045' as a similar designation) for physical constants
1
EOS Aluminium AlSi10Mg Material Data SheetEOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Yield strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Ultimate tensile strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Elongation at break: typical at break, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Thermal conductivity: typical, as manufactured, horizontal (ISO 22007-2)DMLS AlSi10Mg Aluminum · Thermal expansion: mean 25-100 °C, ASTM E228
RenAM 500 Series Aluminium AlSi10Mg Material Data SheetRenishawDMLS AlSi10Mg Aluminum · Young's modulus (stiffness): same material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY)
EOS Aluminium AlSi10Mg Material Data Sheet, FlexLine, M 290 (2018)EOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Density: typical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm)
6
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseDMLS AlSi10Mg Aluminum · Poisson's ratio: base material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000)DMLS AlSi10Mg Aluminum · Specific heat: base material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS AlSi10Mg Aluminum is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS AlSi10Mg Aluminum stronger than Steel AISI 1045?
Steel AISI 1045 is stronger: its yield strength is 531 MPa against 270 MPa for DMLS AlSi10Mg Aluminum (1.97x).
Which is lighter, DMLS AlSi10Mg Aluminum or Steel AISI 1045?
DMLS AlSi10Mg Aluminum is lighter: 2,670 kg/m³ against 7,800 kg/m³ for Steel AISI 1045.
Which is stiffer, DMLS AlSi10Mg Aluminum or Steel AISI 1045?
Steel AISI 1045 is stiffer: Young's modulus 210 GPa against 72 GPa for DMLS AlSi10Mg Aluminum, so the same part in Steel AISI 1045 deflects less under the same load.
Which is lighter for the same job, DMLS AlSi10Mg Aluminum or Steel AISI 1045?
For the same stiffness or strength: DMLS AlSi10Mg Aluminum is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
DMLS AlSi10Mg Aluminum
Steel AISI 1045
Stiff rod or tie (tension)
about equal
about equal
Stiff beam (bending)
lighter
1.71x heavier
Stiff panel or plate
lighter
2.04x heavier
Strong rod or tie
lighter
49% heavier
Strong beam
lighter
1.86x heavier
Strong panel or plate
lighter
2.08x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, DMLS AlSi10Mg Aluminum or Steel AISI 1045?
Steel AISI 1045 stretches further before it breaks: 12% elongation at break against 10.2% for DMLS AlSi10Mg Aluminum.
Thermal
Which conducts heat better, DMLS AlSi10Mg Aluminum or Steel AISI 1045?
DMLS AlSi10Mg Aluminum conducts heat better: 110 W/m·K against 42.5 W/m·K for Steel AISI 1045.
Which expands less with temperature?
Steel AISI 1045 expands less: 12 µm/m·K against 20 µm/m·K for DMLS AlSi10Mg Aluminum.