Materials / Compare

FDM HIPS vs. Plastic PEEK

Compare FDM HIPS vs. Plastic PEEK strength, stiffness, weight and thermal properties.

FDM HIPS3D printed (FDM)
Plastic PEEKBulk polymer (molded or machined)
MechanicalFDM HIPSPlastic PEEK
Yield strengthnot given (tensile used)98MPa1
Ultimate tensile strength18.4MPa2not stated (yield given)
Compressive strengthnot sourced125MPa1
Flexural strength31.8MPa2165MPa1
Elongation at break1.4%225%117.9x more ductile
Young's modulus (stiffness)1.59GPa24GPa12.52x stiffer
Density1,023kg/m³227% lighter1,300kg/m³1
Strength to weight18kN·m/kg75.4kN·m/kg4.19x higher
Stiffness to weight1.55MN·m/kg3.08MN·m/kg1.98x higher
Poisson's rationot sourced0.383
Shear modulusnot sourced1.45GPa
Bulk modulusnot sourced5.56GPa
Speed of sound1,246m/s1,754m/s41% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30FDM HIPSPlastic PEEK
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30FDM HIPSPlastic PEEK
Strength against densityHigher and further left: stronger for its weight
ThermalFDM HIPSPlastic PEEK
Thermal conductivitybase material0.17W/m·K40.29W/m·K11.71x more heat through a fin
Thermal expansionbase material80µm/m·K455µm/m·K145% less
100 mm part over a 50 °C swing400µm growth275µm growth45% less
Specific heatnot sourced2,200J/kg·K5
Heats up and cools (diffusivity)not sourced0.101mm²/s
Thermal shock resistancenot sourced80.1W/m
Melting pointnot sourced343°C1
Glass transition99°C2onset143°C144 °C higher
Max service temperatureHDT 1.8 MPa86°C2UL 746B RTI240°C1
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30FDM HIPSPlastic PEEK
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30FDM HIPSPlastic PEEK
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Victrex, BASF Forward AM, INEOS Styrolution
FDM HIPS
BASF Forward AM (BASF 3D Printing Solutions) Ultrafuse HiPS, TDS v2.2 (13.11.2019), printed specimens, XY 'Flat'. Specimen print settings are not stated; recommended processing on the sheet: nozzle 240-260 °C, bed 100-120 °C, 40-80 mm/s. Product is discontinued (Forward AM product page) but the TDS is still served by Forward AM.
Plastic PEEK
Victrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)
  1. 1
    VICTREX PEEK 450G Technical Data SheetVictrexPlastic PEEK · Yield strength: typical, tensile yieldPlastic PEEK · Compressive strength: typical, 23 CPlastic PEEK · Flexural strength: typical, flexural stress at yield, 23 CPlastic PEEK · Elongation at break: typical, at breakPlastic PEEK · Young's modulus (stiffness): typical (nominal)Plastic PEEK · Density: typical (crystalline)Plastic PEEK · Thermal conductivity: typical, average, 23 CPlastic PEEK · Thermal expansion: average of flow/cross-flow, below Tg (<143 C)Plastic PEEK · Melting point: typical, DSCPlastic PEEK · Glass transition: onset (midpoint 150 C)Plastic PEEK · Max service temperature: UL 746B RTI, mechanical strength (continuous use index)
  2. 2
    Ultrafuse HiPS Technical Data Sheet, v2.2 (2019)BASF Forward AMarchived copyFDM HIPS · Ultimate tensile strength: typicalFDM HIPS · Flexural strength: typicalFDM HIPS · Elongation at break: typicalFDM HIPS · Young's modulus (stiffness): typicalFDM HIPS · Density: typicalFDM HIPS · Glass transition: typicalFDM HIPS · Max service temperature: HDT 1.8 MPa
  3. 3
    VICTREX PEEK for Use in Fluid Management (2020)VictrexPlastic PEEK · Poisson's ratio: typical
  4. 4
    Styrolution PS 486N (HIPS) Product Data SheetINEOS StyrolutionFDM HIPS · Thermal conductivity: base material: INEOS Styrolution PS 486N injection-molding HIPS, typicalFDM HIPS · Thermal expansion: base material: INEOS Styrolution PS 486N injection-molding HIPS, typical
  5. 5
    VICTREX PEEK 450G Technical Data Sheet (2012)Victrexarchived copyPlastic PEEK · Specific heat: typical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM HIPS is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is FDM HIPS stronger than Plastic PEEK?

Plastic PEEK is stronger: its yield strength is 98 MPa against tensile strength 18.4 MPa for FDM HIPS (5.33x).

Which is lighter, FDM HIPS or Plastic PEEK?

FDM HIPS is lighter: 1,023 kg/m³ against 1,300 kg/m³ for Plastic PEEK.

Which is stiffer, FDM HIPS or Plastic PEEK?

Plastic PEEK is stiffer: Young's modulus 4 GPa against 1.59 GPa for FDM HIPS, so the same part in Plastic PEEK deflects less under the same load.

Which is lighter for the same job, FDM HIPS or Plastic PEEK?

For the same stiffness or strength: Plastic PEEK is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beFDM HIPSPlastic PEEK
Stiff rod or tie (tension)1.98x heavierlighter
Stiff beam (bending)25% heavierlighter
Stiff panel or plate7% heavierlighter
Strong rod or tie4.19x heavierlighter
Strong beam2.4x heavierlighter
Strong panel or plate1.82x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, FDM HIPS or Plastic PEEK?

Plastic PEEK stretches further before it breaks: 25% elongation at break against 1.4% for FDM HIPS.

Thermal

Which conducts heat better, FDM HIPS or Plastic PEEK?

Plastic PEEK conducts heat better: 0.29 W/m·K against 0.17 W/m·K for FDM HIPS.

Which expands less with temperature?

Plastic PEEK expands less: 55 µm/m·K against 80 µm/m·K for FDM HIPS.

Related comparisons