Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ31B-H24 · Young's modulus (stiffness): typical (handbook physical constant)Magnesium AZ31B-H24 · Density: nominalMagnesium AZ31B-H24 · Poisson's ratio: typical (handbook physical constant)Magnesium AZ31B-H24 · Max service temperature: stated application limit
4
Eastar Copolyester 6763 Product Data SheetEastmanPlastic PETG · Thermal conductivity: base material: Eastman Eastar Copolyester 6763 (PETG), typicalPlastic PETG · Thermal expansion: base material: Eastman Eastar Copolyester 6763 (PETG), typicalPlastic PETG · Specific heat: base material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Plastic PETG is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Magnesium AZ31B-H24 stronger than Plastic PETG?
Magnesium AZ31B-H24 is stronger: its yield strength is 220 MPa against 46.2 MPa for Plastic PETG (4.76x).
Which is lighter, Magnesium AZ31B-H24 or Plastic PETG?
Plastic PETG is lighter: 1,270 kg/m³ against 1,769 kg/m³ for Magnesium AZ31B-H24.
Which is stiffer, Magnesium AZ31B-H24 or Plastic PETG?
Magnesium AZ31B-H24 is stiffer: Young's modulus 44.8 GPa against 1.94 GPa for Plastic PETG, so the same part in Magnesium AZ31B-H24 deflects less under the same load.
Which is lighter for the same job, Magnesium AZ31B-H24 or Plastic PETG?
For the same stiffness or strength: Magnesium AZ31B-H24 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Magnesium AZ31B-H24
Plastic PETG
Stiff rod or tie (tension)
lighter
16.6x heavier
Stiff beam (bending)
lighter
3.45x heavier
Stiff panel or plate
lighter
2.04x heavier
Strong rod or tie
lighter
3.42x heavier
Strong beam
lighter
2.03x heavier
Strong panel or plate
lighter
1.57x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Magnesium AZ31B-H24 or Plastic PETG?
Magnesium AZ31B-H24 stretches further before it breaks: 13% elongation at break against 7.6% for Plastic PETG.
Thermal
Which conducts heat better, Magnesium AZ31B-H24 or Plastic PETG?
Magnesium AZ31B-H24 conducts heat better: 76.9 W/m·K against 0.21 W/m·K for Plastic PETG.
Which expands less with temperature?
Magnesium AZ31B-H24 expands less: 26.8 µm/m·K against 51 µm/m·K for Plastic PETG.