Materials / Compare

Nickel Inconel 718 vs. Plastic Polycarbonate

Compare Nickel Inconel 718 vs. Plastic Polycarbonate strength, stiffness, weight and thermal properties.

Nickel Inconel 718Wrought
Plastic PolycarbonateBulk polymer (molded or machined)
MechanicalNickel Inconel 718Plastic Polycarbonate
Yield strength1,207MPa118.6x stronger65MPa2
Ultimate tensile strength1,389MPa165MPa2
Flexural strengthnot sourced97MPa2
Elongation at break20%1125%26.25x more ductile
Young's modulus (stiffness)200GPa183.3x stiffer2.4GPa2
Density8,221kg/m³11,200kg/m³26.85x lighter
Strength to weight147kN·m/kg2.71x higher54.2kN·m/kg
Stiffness to weight24.3MN·m/kg12.2x higher2MN·m/kg
Poisson's ratio0.29410.383
Shear modulus77.3GPa88.9x stiffer in shear0.87GPa
Bulk modulus162GPa48.5x higher3.33GPa
Speed of sound4,932m/s3.49x faster1,414m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Nickel Inconel 718Plastic Polycarbonate
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Nickel Inconel 718Plastic Polycarbonate
Strength against densityHigher and further left: stronger for its weight
ThermalNickel Inconel 718Plastic Polycarbonate
Thermal conductivity11.4W/m·K157x more heat through a fin0.2W/m·K2
Thermal expansion13.2µm/m·K14.92x less65µm/m·K2
100 mm part over a 50 °C swing66µm growth4.92x less325µm growth
Specific heat435J/kg·K11,172J/kg·K42.69x higher
Heats up and cools (diffusivity)3.19mm²/s22.4x faster0.142mm²/s
Thermal shock resistance3,680W/m71.2x more resistant51.7W/m
Melting pointmelting range1,260–1,336°C1not sourced
Glass transitionnot sourced144°C2
Max service temperature704°C1579 °C hotterUL 746B RTI125°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Nickel Inconel 718Plastic Polycarbonate
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Nickel Inconel 718Plastic Polycarbonate
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Special Metals, Covestro, Bayer MaterialScience
Nickel Inconel 718
INCONEL alloy 718, standard grade, 1750 °F/1 hr anneal + 1325 °F/8 hr F.C. to 1150 °F aged; Special Metals bulletin SMC-045 typical values
Plastic Polycarbonate
Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values
  1. 1
    INCONEL alloy 718 (SMC-045)Special Metalsarchived copyNickel Inconel 718 · Yield strength: typical, 1.0 in. hot-rolled bar, 0.2% offsetNickel Inconel 718 · Ultimate tensile strength: typical, 1.0 in. barNickel Inconel 718 · Elongation at break: typical, 1.0 in. barNickel Inconel 718 · Young's modulus (stiffness): typical, 21 °C, annealed + agedNickel Inconel 718 · Density: nominal, annealed and agedNickel Inconel 718 · Poisson's ratio: typical, 21 °C, annealed + agedNickel Inconel 718 · Thermal conductivity: typical, 21 °C, annealed + aged (calculated from resistivity per footnote a)Nickel Inconel 718 · Thermal expansion: typical, mean 21-93 °C, annealed + agedNickel Inconel 718 · Specific heat: typical, 21 °CNickel Inconel 718 · Melting point: melting rangeNickel Inconel 718 · Max service temperature: upper use temperature stated by producer
  2. 2
    Makrolon 2405 Technical Data SheetCovestroPlastic Polycarbonate · Yield strength: typical, tensile yieldPlastic Polycarbonate · Ultimate tensile strength: typical, stress at breakPlastic Polycarbonate · Flexural strength: typical, flexural strengthPlastic Polycarbonate · Elongation at break: typical, strain at breakPlastic Polycarbonate · Young's modulus (stiffness): typicalPlastic Polycarbonate · Density: typicalPlastic Polycarbonate · Thermal conductivity: typical, through-plane, 23 CPlastic Polycarbonate · Thermal expansion: typical, 23-55 C, parallel and normalPlastic Polycarbonate · Glass transition: typical, DSC 10 C/minPlastic Polycarbonate · Max service temperature: UL 746B RTI, tensile strength, 1.5 mm
  3. 3
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic Polycarbonate · Poisson's ratio: typical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
  4. 4
    Makrolon 2405 Data Sheet, ASTM valuesBayer MaterialSciencearchived copyPlastic Polycarbonate · Specific heat: typical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Nickel Inconel 718 stronger than Plastic Polycarbonate?

Nickel Inconel 718 is stronger: its yield strength is 1,207 MPa against 65 MPa for Plastic Polycarbonate (18.6x).

Which is lighter, Nickel Inconel 718 or Plastic Polycarbonate?

Plastic Polycarbonate is lighter: 1,200 kg/m³ against 8,221 kg/m³ for Nickel Inconel 718.

Which is stiffer, Nickel Inconel 718 or Plastic Polycarbonate?

Nickel Inconel 718 is stiffer: Young's modulus 200 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Nickel Inconel 718 deflects less under the same load.

Which is lighter for the same job, Nickel Inconel 718 or Plastic Polycarbonate?

For the same stiffness or strength: Nickel Inconel 718 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam; Plastic Polycarbonate is lighter for a stiff panel or plate, strong panel or plate.

Part that must beNickel Inconel 718Plastic Polycarbonate
Stiff rod or tie (tension)lighter12.2x heavier
Stiff beam (bending)lighter33% heavier
Stiff panel or plate1.57x heavierlighter
Strong rod or tielighter2.71x heavier
Strong beamlighter2% heavier
Strong panel or plate1.59x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Nickel Inconel 718 or Plastic Polycarbonate?

Plastic Polycarbonate stretches further before it breaks: 125% elongation at break against 20% for Nickel Inconel 718.

Thermal

Which handles higher temperatures, Nickel Inconel 718 or Plastic Polycarbonate?

Nickel Inconel 718 does: 704 °C against 125 °C for Plastic Polycarbonate.

Which conducts heat better, Nickel Inconel 718 or Plastic Polycarbonate?

Nickel Inconel 718 conducts heat better: 11.4 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.

Which expands less with temperature?

Nickel Inconel 718 expands less: 13.2 µm/m·K against 65 µm/m·K for Plastic Polycarbonate.

Related comparisons