Plastic ABS3D printed (FDM)
Plastic Nylon3D printed (FDM)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength38.1MPasourcetypical63.1MPasourcetypical1.66x stronger
Ultimate tensile strength38.1MPasourcetypical, peak stress (= stress at yield)63.1MPasourcetypical, peak stress (= stress at yield)1.66x stronger
Flexural strength61.1MPasourcetypical82.9MPasourcetypical36% stronger in bending
Elongation at break4.6%sourcetypicalnot sourced
Young's modulus (stiffness)1.96GPasourcetypical2.33GPasourcetypical19% stiffer
Density1,100kg/m³sourcetypical1,140kg/m³sourcetypical
Strength to weight34.6kN·m/kg55.4kN·m/kg1.6x higher
Stiffness to weight1.78MN·m/kg2.04MN·m/kg15% higher
Poisson's ratio0.39sourcebase material: ABS family typical (Covestro Part and Mold Design guide, Table 3-1)0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
Shear modulus0.706GPa0.833GPa18% stiffer in shear
Bulk modulus2.97GPa3.89GPa
Speed of sound1,336m/s1,430m/s
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, typical0.33W/m·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, range98–102µm/m·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K, 98) and PA6 (B3S, 102), 23-55 C
100 mm part over a 50 °C swing475µm growth5% less500µm growth
Specific heatnot sourced1,700J/kg·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)
Heats up and cools (diffusivity)not sourced0.17mm²/s
Thermal shock resistance21.2W/m53.6W/m2.53x more resistant
Melting pointnot sourced188°Csourcetypical
Glass transition101°Csourcetypical55.1°Csourcetypical
Max service temperature86.6°CsourceHDT 0.455 MPa (printed specimens)89.2°CsourceHDT 0.455 MPa (printed specimens)
Values forUltimaker ABS, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v5.00, April 20, 2022.Ultimaker Nylon, 3D-printed specimens, XY (flat), conditioned >=24 h at room temperature; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v2.00, April 20, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic ABS and Plastic Nylon are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic ABS stronger than Plastic Nylon?

Plastic Nylon is stronger: its yield strength is 63.1 MPa against 38.1 MPa for Plastic ABS (1.66x).

Which is lighter, Plastic ABS or Plastic Nylon?

Plastic ABS is lighter: 1,100 kg/m³ against 1,140 kg/m³ for Plastic Nylon.

Which is stiffer, Plastic ABS or Plastic Nylon?

Plastic Nylon is stiffer: Young's modulus 2.33 GPa against 1.96 GPa for Plastic ABS, so the same part in Plastic Nylon deflects less under the same load.

Which is lighter for the same job, Plastic ABS or Plastic Nylon?

For the same stiffness or strength: Plastic Nylon is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABSPlastic Nylon
Stiff rod or tie (tension)15% heavierlighter
Stiff beam (bending)5% heavierlighter
Stiff panel or plate2% heavierlighter
Strong rod or tie1.6x heavierlighter
Strong beam35% heavierlighter
Strong panel or plate24% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic ABS or Plastic Nylon?

Plastic Nylon conducts heat better: 0.33 W/m·K against 0.17 W/m·K for Plastic ABS.

Which expands less with temperature?

Plastic ABS expands less: 95 µm/m·K against 100 µm/m·K for Plastic Nylon.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic TPUAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABSPlastic Nylon
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic TPURubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABSPlastic Nylon
Strength against density