Materials / Compare

Plastic ABS vs. Plastic PEEK

Compare Plastic ABS vs. Plastic PEEK strength, stiffness, weight and thermal properties.

Change either side
Plastic ABS3D printed (FDM)
Plastic PEEKBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength38.1MPasourcetypical98MPasourcetypical, tensile yield
Ultimate tensile strength38.1MPasourcetypical, peak stress (= stress at yield)not sourced
Compressive strengthnot sourced125MPasourcetypical, 23 C
Flexural strength61.1MPasourcetypical165MPasourcetypical, flexural stress at yield, 23 C
Elongation at break4.6%sourcetypical25%sourcetypical, at break
Young's modulus (stiffness)1.96GPasourcetypical4GPasourcetypical (nominal)
Density1,100kg/m³sourcetypical1,300kg/m³sourcetypical (crystalline)
Strength to weight34.6kN·m/kg75.4kN·m/kg2.18x higher
Stiffness to weight1.78MN·m/kg3.08MN·m/kg1.73x higher
Poisson's ratio0.39sourcebase material: ABS family typical (Covestro Part and Mold Design guide, Table 3-1)0.38sourcetypical
Shear modulus0.706GPa1.45GPa2.05x stiffer in shear
Bulk modulus2.97GPa5.56GPa
Speed of sound1,336m/s1,754m/s
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, typical0.29W/m·Ksourcetypical, average, 23 C
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, range55µm/m·Ksourceaverage of flow/cross-flow, below Tg (<143 C)
100 mm part over a 50 °C swing475µm growth275µm growth1.73x less
Specific heatnot sourced2,200J/kg·Ksourcetypical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)
Heats up and cools (diffusivity)not sourced0.101mm²/s
Thermal shock resistance21.2W/m80.1W/m3.78x more resistant
Melting pointnot sourced343°Csourcetypical, DSC
Glass transition101°Csourcetypical143°Csourceonset (midpoint 150 C)
Max service temperature86.6°CsourceHDT 0.455 MPa (printed specimens)240°CsourceUL 746B RTI, mechanical strength (continuous use index)
Values forUltimaker ABS, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v5.00, April 20, 2022.Victrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic ABS is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic ABS stronger than Plastic PEEK?

Plastic PEEK is stronger: its yield strength is 98 MPa against 38.1 MPa for Plastic ABS (2.57x).

Which is lighter, Plastic ABS or Plastic PEEK?

Plastic ABS is lighter: 1,100 kg/m³ against 1,300 kg/m³ for Plastic PEEK.

Which is stiffer, Plastic ABS or Plastic PEEK?

Plastic PEEK is stiffer: Young's modulus 4 GPa against 1.96 GPa for Plastic ABS, so the same part in Plastic PEEK deflects less under the same load.

Which is lighter for the same job, Plastic ABS or Plastic PEEK?

For the same stiffness or strength: Plastic PEEK is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABSPlastic PEEK
Stiff rod or tie (tension)1.73x heavierlighter
Stiff beam (bending)21% heavierlighter
Stiff panel or plate7% heavierlighter
Strong rod or tie2.18x heavierlighter
Strong beam1.59x heavierlighter
Strong panel or plate36% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic ABS or Plastic PEEK?

Plastic PEEK conducts heat better: 0.29 W/m·K against 0.17 W/m·K for Plastic ABS.

Which expands less with temperature?

Plastic PEEK expands less: 55 µm/m·K against 95 µm/m·K for Plastic ABS.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABSPlastic PEEK
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABSPlastic PEEK
Strength against density

Related comparisons