Materials / Compare

Plastic Nylon PA6 vs. Plastic PETG

Compare Plastic Nylon PA6 vs. Plastic PETG strength, stiffness, weight and thermal properties.

Change either side
Plastic Nylon PA6Bulk polymer (molded or machined)
Plastic PETG3D printed (FDM)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength90MPasourcetypical, dry46.2MPasourcetypical
Ultimate tensile strengthnot sourced46.2MPasourcetypical, peak stress (= stress at yield)
Flexural strengthnot sourced78.9MPasourcetypical
Elongation at break10%sourcenominal strain at break, dry7.6%sourcetypical
Young's modulus (stiffness)3.5GPasourcetypical, dry1.94GPasourcetypical
Density1,130kg/m³sourcetypical12% lighter1,270kg/m³sourcetypical
Strength to weight79.6kN·m/kg2.19x higher36.4kN·m/kg
Stiffness to weight3.1MN·m/kg2.03x higher1.53MN·m/kg
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)not sourced
Shear modulus1.25GPanot sourced
Bulk modulus5.83GPanot sourced
Speed of sound1,760m/s1,236m/s
Thermal
Thermal conductivity0.33W/m·Ksourcetypical0.21W/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical
Thermal expansion102µm/m·Ksourcelongitudinal, 23-55 °C51µm/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical
100 mm part over a 50 °C swing510µm growth255µm growth2x less
Specific heat1,700J/kg·Ksourcetypical1,300J/kg·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)
Heats up and cools (diffusivity)0.172mm²/s35% faster0.127mm²/s
Thermal shock resistance49.9W/mnot sourced
Melting point220°CsourceDSCnot sourced
Glass transitionnot sourced77.4°Csourcetypical
Max service temperature87°CsourceIEC 60216 temperature index, 20000 h76.2°CsourceHDT 0.455 MPa (printed specimens)
Values forBASF Ultramid B3S (PA6, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)Ultimaker PETG, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v1.00, April 29, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PETG is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic Nylon PA6 stronger than Plastic PETG?

Plastic Nylon PA6 is stronger: its yield strength is 90 MPa against 46.2 MPa for Plastic PETG (1.95x).

Which is lighter, Plastic Nylon PA6 or Plastic PETG?

Plastic Nylon PA6 is lighter: 1,130 kg/m³ against 1,270 kg/m³ for Plastic PETG.

Which is stiffer, Plastic Nylon PA6 or Plastic PETG?

Plastic Nylon PA6 is stiffer: Young's modulus 3.5 GPa against 1.94 GPa for Plastic PETG, so the same part in Plastic Nylon PA6 deflects less under the same load.

Which is lighter for the same job, Plastic Nylon PA6 or Plastic PETG?

For the same stiffness or strength: Plastic Nylon PA6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic Nylon PA6Plastic PETG
Stiff rod or tie (tension)lighter2.03x heavier
Stiff beam (bending)lighter1.51x heavier
Stiff panel or platelighter37% heavier
Strong rod or tielighter2.19x heavier
Strong beamlighter1.75x heavier
Strong panel or platelighter1.57x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic Nylon PA6 or Plastic PETG?

Plastic Nylon PA6 conducts heat better: 0.33 W/m·K against 0.21 W/m·K for Plastic PETG.

Which expands less with temperature?

Plastic PETG expands less: 51 µm/m·K against 102 µm/m·K for Plastic Nylon PA6.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Nylon PA6Plastic PETG
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic Nylon PA6Plastic PETG
Strength against density