Materials / Compare

Plastic Nylon vs. Plastic PMMA

Compare Plastic Nylon vs. Plastic PMMA strength, stiffness, weight and thermal properties.

Change either side
Plastic Nylon3D printed (FDM)
Plastic PMMABulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength63.1MPasourcetypicalnot given (tensile used)
Ultimate tensile strength63.1MPasourcetypical, peak stress (= stress at yield)80MPasourcetypical, 23 °C
Compressive strengthnot sourced110MPasourcecompressive yield stress, typical
Flexural strength82.9MPasourcetypical115MPasourcetypical39% stronger in bending
Elongation at breaknot sourced5.5%sourcetypical
Young's modulus (stiffness)2.33GPasourcetypical3.3GPasourcetypical, short-term
Density1,140kg/m³sourcetypical1,190kg/m³sourcetypical
Strength to weight55.4kN·m/kg67.2kN·m/kg21% higher
Stiffness to weight2.04MN·m/kg2.77MN·m/kg36% higher
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)0.37sourcetypical
Shear modulus0.833GPa1.2GPa45% stiffer in shear
Bulk modulus3.89GPa4.23GPa
Speed of sound1,430m/s1,665m/s
Thermal
Thermal conductivity0.33W/m·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)0.19W/m·Ksourcetypical
Thermal expansion98–102µm/m·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K, 98) and PA6 (B3S, 102), 23-55 C70µm/m·Ksource0-50 °C
100 mm part over a 50 °C swing500µm growth350µm growth43% less
Specific heat1,700J/kg·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)1,470J/kg·Ksourcetypical
Heats up and cools (diffusivity)0.17mm²/s1.57x faster0.109mm²/s
Thermal shock resistance53.6W/m29% more resistant41.5W/m
Melting point188°Csourcetypicalnot sourced
Glass transition55.1°Csourcetypicalnot sourced
Max service temperature89.2°CsourceHDT 0.455 MPa (printed specimens)80°Csourcemax. permanent service temperature
Values forUltimaker Nylon, 3D-printed specimens, XY (flat), conditioned >=24 h at room temperature; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v2.00, April 20, 2022.Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic Nylon stronger than Plastic PMMA?

Plastic PMMA is stronger: its tensile strength is 80 MPa against yield strength 63.1 MPa for Plastic Nylon (27%).

Which is lighter, Plastic Nylon or Plastic PMMA?

Plastic Nylon is lighter: 1,140 kg/m³ against 1,190 kg/m³ for Plastic PMMA.

Which is stiffer, Plastic Nylon or Plastic PMMA?

Plastic PMMA is stiffer: Young's modulus 3.3 GPa against 2.33 GPa for Plastic Nylon, so the same part in Plastic PMMA deflects less under the same load.

Which is lighter for the same job, Plastic Nylon or Plastic PMMA?

For the same stiffness or strength: Plastic PMMA is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic NylonPlastic PMMA
Stiff rod or tie (tension)36% heavierlighter
Stiff beam (bending)14% heavierlighter
Stiff panel or plate8% heavierlighter
Strong rod or tie21% heavierlighter
Strong beam12% heavierlighter
Strong panel or plate8% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic Nylon or Plastic PMMA?

Plastic Nylon conducts heat better: 0.33 W/m·K against 0.19 W/m·K for Plastic PMMA.

Which expands less with temperature?

Plastic PMMA expands less: 70 µm/m·K against 100 µm/m·K for Plastic Nylon.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic NylonPlastic PMMA
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPURubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic NylonPlastic PMMA
Strength against density

Related comparisons